Alloy Digest (2017) 66 (9): TS-741.
Published: 01 September 2017
... Böhler (or Boehler) S200 is a high-speed steel with good toughness and red hardness. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on surface qualities as well as forming, heat treating, and machining. Filing Code...