Alloy Digest (2007) 56 (10): TS-656.
Published: 01 October 2007
... Boehler S790 Microclean is a high-speed steel produced by powder metallurgy techniques. It has good red hardness and compressive stress resistance. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming and heat treating...