Skip Nav Destination
Close Modal
Search Results for
Boehler M310 ISOPLAST
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
Boehler M310 ISOPLAST
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2000) 49 (5): TS-577.
Published: 01 May 2000
... Boehler M310 ISOPLAST is a martensitic stainless steel encompassing specialized thermal treatments and electroslag remelting to develop a plastic mold alloy with a combination of properties including corrosion and wear resistance and polishability. This datasheet provides information...
Abstract
View article
PDF
Boehler M310 ISOPLAST is a martensitic stainless steel encompassing specialized thermal treatments and electroslag remelting to develop a plastic mold alloy with a combination of properties including corrosion and wear resistance and polishability. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating, machining, and joining. Filing Code: TS-577. Producer or source: Böhler.