Alloy Digest (2004) 53 (10): TS-607.
Published: 01 October 2004
... Boehler K390 Microclean is a cold work tool steel with an extremely good wear resistance combined with good toughness and a high compressive strength. This alloy is of powder metallurgical origins and is very homogeneous. This datasheet provides information on composition, physical properties...