1-20 of 27 Search Results for

Bethlehem V steel

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1970) 19 (10): SA-257.
Published: 01 October 1970
... BETHLEHEM V STEEL comprises a family of high-strength, low-alloy, hot-rolled steels in various forms for construction and general purposes. These steels offer yield strengths ranging from 42,000 to 65,000 psi. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1989) 38 (7): SA-438.
Published: 01 July 1989
... BETHLEHEM V-STAR 50 is an as-rolled steel for and H-and sheet piling sections. It offers the design benefits of high-strength steel economically. It is particularly good where impact loading is encountered. It is readily weldable using conventional welding processes. This datasheet provides...
Journal Articles
Alloy Digest (1977) 26 (2): TS-313.
Published: 01 February 1977
... will withstand drastic cooling from maximum operating temperatures. *CROMO-V is a registered trademark of Bethlehem Steel Corporation. Composition: Typical Carbon 0.40 Silicon 0.90 Chromium 5 .oo Molybdenum 1.30 Vanadium 0.50 PROPERTIES Table 1 - EFFECT OF AUSTENITIZING TEMPERATURE AND TYPE OF COOLING...
Journal Articles
Alloy Digest (1973) 22 (5): TS-254.
Published: 01 May 1973
... Cromo-High V is a 5% chromium-molydbenum-vanadium tool steel that is used widely in the die-casting industry. It has high red-hardness with good resistance to abrasion and heat checking. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1972) 21 (3): SA-272.
Published: 01 March 1972
... BETHLEHEM RQ-100A is a heat-treated alloy steel having 100,000 psi yield strength through 11/4-in. thickness, in combination with good toughness, abrasion resistance and weldability. It is engineered specifically for structural applications such as earth moving equipment,buildings, bridges, and...
Journal Articles
Alloy Digest (2000) 49 (12): SA-506.
Published: 01 December 2000
... BETHLEHEM LUKENS PLATE HPS-70W is a high-performance steel (HPS) developed through a cooperative agreement among the Federal Highway Administration (FHWA), the American Iron and Steel Institute (AISI), and the Department of the Navy. This steel is an improved version of ASTM A 709 grade 70W. This...
Journal Articles
Alloy Digest (1971) 20 (9): CS-43.
Published: 01 September 1971
... BETHLEHEM RQC-80 is a heat-treated carbon steel having 80,000 psi yield strength through 11/2-in. plate, in combination with good notch toughness and excellent weldability. It is engineered specifically for structural applications such as drilling rigs, earthmoving machinery, railroad cars, and...
Journal Articles
Alloy Digest (1971) 20 (12): CS-45.
Published: 01 December 1971
... BETHLEHEM RQC-90 is a roller quenched and tempered carbon steel with a 90,000 psi yield strength combined with good notch toughness and weldability. It is available in thicknesses through 11/2 inches. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (1956) 5 (7): TS-48.
Published: 01 July 1956
... WORLD WIDE METALS AND ALLOYS Pabkbd b-v Enginecriug Alloys bigest, Inc. Upper Montclair, New Jersey BETHLEHEM 67 CHISEL (Shock Resistant Tool Steel Type Sl) BEllWSEM 67 CHISEL is tbe general-purpose, tungsten-We of sbodr-resisting tool steel. It has excellent properties for cold batter- ing tools and...
Journal Articles
Alloy Digest (1957) 6 (4): TS-57.
Published: 01 April 1957
... composition fracture toughness hardness heat treatability high-temperature alloys machinability shock resistance tensile properties wear resistance workability v BETHLEHEM Cr-MO-W Filing Code: TS-57 Tool Steel APRIL 1957 DIGESTa - DATA ON WORLD WIDE METALS AND ALLOYS ~P*blisbd by. z-- D- = I New...
Journal Articles
Alloy Digest (1971) 20 (7): CS-42.
Published: 01 July 1971
... BETHLEHEM RQC-60 is a heat-treated carbon steel having up to 60,000 psi yield strength in combination with good notch toughness and excellent weldability. It is engineered specifically for pressure vessels, storage tanks, and structures where low-temperature service is required. This datasheet...
Journal Articles
Alloy Digest (2003) 52 (8): SA-518.
Published: 01 August 2003
... Bethlehem Lukens Plate (BLP) offers five grades of Spartan high-strength steels with tensile yield strength over 690 MPa (100 ksi). These alloys contain copper for precipitation reactions. They also have improved weldability and toughness compared to ASTM A 514 and A 543 grades. This datasheet...
Journal Articles
Alloy Digest (1992) 41 (1): SA-383.
Published: 01 January 1992
... BETHLEHEM HOT-ROLLED SHEET XF SERIES alloys B50XF, B60XF, B70XF and B80XF are high strength low alloy steels. The numbers in the alloy designations refer to minimum yield strengths. The steels are made using ladle desulfurization which virtually eliminates harmful stringer type inclusions. The...
Journal Articles
Alloy Digest (1962) 11 (1): TS-113.
Published: 01 January 1962
... Hotform V is a medium-carbon, 5% chromium hot work tool and die steel having improved wear resistance and hot hardness at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (2003) 52 (9): SA-520.
Published: 01 September 2003
... values correspond with the typical range most commonly used for plates produced by Bethlehem Lukens Plate. The commonly used International Institute of Welding Carbon Equivalent (IIW C.E.) is based on the empirical equation: CE = C+ (Mn/6) + (Cr + Mo + V/5) + (Ni + Cu/15) For steels with lower carbon...
Journal Articles
Alloy Digest (2001) 50 (1): SS-815.
Published: 01 January 2001
... UNS S41003 is a low-cost utilitarian martensitic stainless steel to be used for highway and other applications. It is used in the tempered condition at several strength levels. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear and...
Journal Articles
Alloy Digest (1986) 35 (8): SA-421.
Published: 01 August 1986
... information on forming, heat treating, and joining. Filing Code: SA-421. Producer or source: Bethlehem Steel Corporation. Producer or Source: Bethlehem Steel Corporation Copyright © ASM International® 1996 1996 ASM International BETHSTAR 60 chemical composition elasticity fracture toughness...
Journal Articles
Alloy Digest (1982) 31 (7): SA-385.
Published: 01 July 1982
..., and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-385. Producer or source: Bethlehem Steel Corporation. Producer or Source: Bethlehem Steel Corporation Copyright © ASM International® 1996 1996...
Journal Articles
Alloy Digest (1990) 39 (4): SA-446.
Published: 01 April 1990
... Code: SA-446. Producer or source: Bethlehem Steel Corporation. Producer or Source: Bethlehem Steel Corporation Copyright © ASM International® 1996 1996 ASM International ASTM A710 chemical composition fracture toughness heat treatability joinability tensile properties UNS K20747...
Journal Articles
Alloy Digest (2003) 52 (10): SA-522.
Published: 01 October 2003
... BethStar 70 steel plate is a high-strength product with a 483 MPa (70 ksi) minimum yield strength. It contains low carbon and low sulfur and has outstanding toughness, weldability, and formability. It provides the design engineer with an option in an economical high-strength low-alloy (HSLA) grade...