Skip Nav Destination
Close Modal
Search Results for
Bethlehem RQ-100A
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
Bethlehem RQ-100A
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1968) 17 (1): SA-221.
Published: 01 January 1968
... Bethlehem RQ-100A is a roller-quenched and tempered constructional alloy steel for applications such as bridges, buildings, derricks, mining equipment, earth moving equipment, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Abstract
View article
PDF
Bethlehem RQ-100A is a roller-quenched and tempered constructional alloy steel for applications such as bridges, buildings, derricks, mining equipment, earth moving equipment, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-221. Producer or source: Bethlehem Steel Corporation. See also Alloy Digest SA-272, March 1972.
Journal Articles
Alloy Digest (1972) 21 (3): SA-272.
Published: 01 March 1972
... BETHLEHEM RQ-100A is a heat-treated alloy steel having 100,000 psi yield strength through 11/4-in. thickness, in combination with good toughness, abrasion resistance and weldability. It is engineered specifically for structural applications such as earth moving equipment,buildings, bridges...
Abstract
View article
PDF
BETHLEHEM RQ-100A is a heat-treated alloy steel having 100,000 psi yield strength through 11/4-in. thickness, in combination with good toughness, abrasion resistance and weldability. It is engineered specifically for structural applications such as earth moving equipment,buildings, bridges, and pressure vessels where high strength is required. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-272. Producer or source: Bethlehem Steel Corporation. See also Alloy Digest SA-221, January 1968.