Skip Nav Destination
Close Modal
Search Results for
BethStar 70
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-4 of 4 Search Results for
BethStar 70
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (10): SA-522.
Published: 01 October 2003
... BethStar 70 steel plate is a high-strength product with a 483 MPa (70 ksi) minimum yield strength. It contains low carbon and low sulfur and has outstanding toughness, weldability, and formability. It provides the design engineer with an option in an economical high-strength low-alloy (HSLA) grade...
Abstract
View article
PDF
BethStar 70 steel plate is a high-strength product with a 483 MPa (70 ksi) minimum yield strength. It contains low carbon and low sulfur and has outstanding toughness, weldability, and formability. It provides the design engineer with an option in an economical high-strength low-alloy (HSLA) grade by being one of a family of alloy that can be fabricated readily. Applications include weight-sensitive components subject to high stress such as frames for large off-highway equipment. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-522. Producer or source: Bethlehem Lukens Plate.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (8): SA-421.
Published: 01 August 1986
... BethStar 60 steel plate is a high-strength product with a 60,000 psi minimum yield strength. It contains low carbon and low sulfur and has outstanding toughness, weldability and formability. It provides the design engineer with a an economical high-strength low-alloy (HSLA) grade that can...
Abstract
View article
PDF
BethStar 60 steel plate is a high-strength product with a 60,000 psi minimum yield strength. It contains low carbon and low sulfur and has outstanding toughness, weldability and formability. It provides the design engineer with a an economical high-strength low-alloy (HSLA) grade that can be fabricated readily. Applications include weight-sensitive components subject to high stress such as frames for large off-highway haulers. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-421. Producer or source: Bethlehem Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (7): SA-385.
Published: 01 July 1982
... at 550°F + stress relieved I hour at 1100°F. I.e.2 I go- go- 70- Manual ElOOl8 35 kJi TEMPERATURE, F Heat Treatment: BethStar 80 plate is used in the as-rolled condition. The rolling is controlled (proprietary) processing which contributes to the excel- lent mechanical properties of this steel...
Abstract
View article
PDF
BETHSTAR 80 steel plate is a high-strength product with an 80,000 psi minimum yield strength. It attains this strength in the as-rolled condition through the combination of a low-carbon microalloyed chemistry and controlled (proprietary) processing. It offers substantial cost savings when compared with quenched-and-tempered steel plate. BethStar 80 plate can be machined, formed and welded readily. It is used in several constructional applications and has the potential for many more applications. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-385. Producer or source: Bethlehem Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (9): SA-520.
Published: 01 September 2003
...), J/kg K (Btu/lb °F) Coefficient of linear thermal expansion, 10 6/K (10 6/°F) 21 100 °C (70 212 °F) 12.4 (6.9) 21 316 °C (70 600 °F) 13.5 (7.5) 21 538 °C (70 1000 °F) 14.4 (8.0) Mechanical Properties: See Table 1. Heat Treatment: BethStar 50 plate is used in the as-rolled condition. The rolling...
Abstract
View article
PDF
BethStar 50 steel plate is a high-strength product with a 345 MPa (50 ksi) minimum yield strength. It contains low carbon and low sulfur and has outstanding toughness, weldability, and formability. It provides options for off-highway equipment. This datasheet provides information on composition, physical properties, microstructure, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-520. Producer or source: Bethlehem Lukens Plate.