1-2 of 2 Search Results for

Berylco PS-20

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1972) 21 (8): Be-2.
Published: 01 August 1972
... BERYLCO PS-20 is beryllium sheet produced by rolling slabs of hot-pressed beryllium powder, PR-20 is the designation of the same composition rolled to plate. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1952) 1 (3): Cu-3.
Published: 01 November 1952
... Berylco 25S alloy is the high-performance beryllium-copper spring material of 2 percent nominal beryllium content. It responds to precipitation-hardening for maximum mechanical properties. It has high elastic and endurance strength, good electrical and thermal conductivity, excellent resistance...