Alloy Digest (1954) 3 (7): Cu-18.
Published: 01 July 1954
... Berylco 20CR is the most widely used high strength beryllium copper casting alloy. This alloy can be heat treated to high hardness and tensile strengths; it has high impact strength and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness...