Alloy Digest (1992) 41 (7): Cu-574.
Published: 01 July 1992
... BRUSH CASTING ALLOY 3C is in the beryllium copper family, offering high thermal and electrical conductivity with moderate strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, heat...
Journal Articles
Alloy Digest (1983) 32 (3): Cu-454.
Published: 01 March 1983
... limited cold working can be done on rod and bar; however, a coaJiderable amount of cold working and forming can be done on strip and wire. The manufacturer can supply much more information on the cold workability of this alloy. Casting Characteristics: Brush Alloy 3 (designated 3C in castings) can be cast...
Journal Articles
Alloy Digest (1996) 45 (4): Ni-506.
Published: 01 April 1996
... National NUKOO Radiac SCdiOg SC5 36K5 WI C-361H8-V32 C-KUGS-V32 -JW. 37~JVK C4&JlCV4 GsH&Vl~P C6o-G9-vm-P SC5 36K5 VUI SC5 36L4 VUI SCS36LAVUl 5OA36lG7B24 C46lJ5-V32 3C-6OH6-V3 c-8OJ%V32 SOA361H7B24 3C-8016V32 3cmG7-v32 3C-12OH8-V32 3c-12OG8-v32 C46G7-BA 1 GC46-I15V GCS4-J15V GCS4-JlN GCSON- lOV7 GC&J-VS...