Alloy Digest (1983) 32 (3): Cu-454.
Published: 01 March 1983
... BRUSH Alloy 3 offers the highest electrical and thermal conductivity of any beryllium-copper alloy. It possesses an excellent combination of moderate strength, good corrosion resistance and good resistance to moderately elevated temperatures. Because of its unique physical and mechanical...
Journal Articles
Alloy Digest (1975) 24 (9): Al-217.
Published: 01 September 1975
... BRUSH WELLMAN ALLOY D7 is a beryllium-containing aluminum casting alloy developed primarily as a plastic tooling material. Its main advantages are: (1) Excellent replication of detail, (2) High hardness and (3) Aging at room temperature. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1992) 41 (7): Cu-573.
Published: 01 July 1992
... B50-60 AsCast&Aged 25-45 170-310 55-70 380-480 lo-15 B65-75 Solution Annealed & Aged 70-80 480-550 go-110 620-760 3-15 B92-100 Table 2 - MELTING AND POURING RANGES Solidus Liquidus Pouring Range OF C F C F C Brush Alloy 1OC 1830 1000 1890 1030 2000-2150 1090-1180 DOI: 10.31399/asm.ad.cu0573...
Journal Articles
Alloy Digest (1992) 41 (7): Cu-574.
Published: 01 July 1992
...-520 1 O-20 B75-90 Solution Annealed & Aged 70-80 480-550 90-110 620-690 5-10 B92-100 Table 2 - MELTING AND POURING RANGES Solidus Liquidus Pouring Range F C OF C F C Brush Alloy 3C 1900 1040 1970 1080 2000-2150 1090-l 180 DOI: 10.31399/asm.ad.cu0574 Copyright © ASM International® 1996 Table 3...
Journal Articles
Alloy Digest (1992) 41 (8): Cu-575.
Published: 01 August 1992
...-24 Solution Annealed & Aged 120-150 830-1030 150-175 1030-1210 l-3 C38-43 Table 2 - MELTING AND POURING RANGES Brush Alloy 21C Solidus Liquidus Pouring Range F C F C F C - - - - 1550 840 1760 960 1850-2050 1010-1120 DOI: 10.31399/asm.ad.cu0575 Copyright © ASM International® 1996 Table 3...
Journal Articles
Alloy Digest (1968) 17 (9): Ni-138.
Published: 01 September 1968
... Brush Alloy 260-C is a beryllium nickel casting alloy having high strength, hardness and good corrosion resistance. It is recommended for fuel pump impellers, turbines, non-sparking tools, molds for plastics and glass. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1968) 17 (5): Cu-187.
Published: 01 May 1968
... BRUSH Alloy 10 is a low beryllium, cobalt-bearing copper alloy offering an excellent combination of strength, toughness and conductivity due to an age-hardening heat treatment. It is recommended for springs, clutch rings, resistance welding electrodes and tips, etc. This datasheet provides...
Journal Articles
Alloy Digest (1987) 36 (12): Cu-532.
Published: 01 December 1987
...° F for 2-3 hours, air cool. Protective atmosphere not required unless bright finish without cleaning is specified. Properties are greatly enhanced if material is cold worked prior to aging (see Fig. I). Machining: Machinability of Brush Alloy 165 in the solution-annealed or cold- worked condition is...
Journal Articles
Alloy Digest (1992) 41 (11): Cu-578.
Published: 01 November 1992
... BRUSH WELLMAN Alloy 174 is a beryllium copper alloy with cobalt designed to be a current-carrying component where high strength and relaxation resistance alloys are needed for body downsizing and miniaturization of microprocessors. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1969) 18 (2): Ni-142.
Published: 01 February 1969
... Company. Producer or Source: Brush Beryllium Company Copyright © ASM International® 1996 1996 ASM International BRUSH Alloy 200C castability chemical composition corrosion-resistant alloys elasticity fracture toughness fuel pump impellers hardness heat treatability high-temperature...
Journal Articles
Alloy Digest (1966) 15 (7): Ni-114.
Published: 01 July 1966
... Brush Alloy M220C is a betyllium-nickel casting alloy that responds to an age-hardening heat treatment and is characterized by high strength thermal conductivity combined with excellent corrosion, oxidation and wear resistance. It is recommended for mold tooling in the glass industries. This...
Journal Articles
Alloy Digest (1986) 35 (5): Cu-509.
Published: 01 May 1986
... BRUSH ALLOY 174 beryllium copper is a family of alloys designed to allow denser packaging, miniaturization, higher currents and higher operating temperatures in electrical and electronic applications. It offers improved electrical and thermal conductivity, superior resistance to stress relaxation...
Journal Articles
Alloy Digest (2004) 53 (3): Cu-712.
Published: 01 March 2004
... Brush Alloy 390 was specifically designed for high-power applications and provides a combination of high strength and high conductivity. Increasing power requirements drive the need for lower conductor resistance to reduce joule heating. This alloy has a high thermal conductivity that is critical...
Journal Articles
Alloy Digest (1978) 27 (6): Cu-356.
Published: 01 June 1978
... BRUSH Alloy 25 attains the highest strength and hardness of any copper-base alloy. In the age-hardened condition, its tensile strength can exceed 200,000 psi and its Rockwell C hardness can reach 45. Its many applications include springs, deep-drawing parts, current-carrying springs connectors...
Journal Articles
Alloy Digest (1968) 17 (12): Cu-194.
Published: 01 December 1968
... Brush Alloy 190 is a mill-heat treated beryllium copper strip with a tensile strength up to 190,000 psi. It eliminates the need of customer heat-treating by providing high properties combined with exceptional formability. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1987) 36 (1): Be-3.
Published: 01 January 1987
... treatment. Filing Code: Be-3. Producer or source: Brush Wellman Inc.. Producer or Source: Brush Wellman Inc. Copyright © ASM International® 1996 1996 ASM International aerospace structures applications BRUSH WELLMAN S-65B chemical composition corrosion-resistant alloys ductility elasticity...
Journal Articles
Alloy Digest (1992) 41 (10): Cu-577.
Published: 01 October 1992
...-180 1140-1240 l-2 c40-45 Table 2 - MELTING AND POURING RANGES Brush Alloys 245C and 245C-f Solidus Liquidus Pouring Range F C F C F C - - 1585 860 1750 955 1775-1950 970-1070 DOI: 10.31399/asm.ad.cu0577 Copyright © ASM International® 1996 Table 3 -RECOMMENDED MACHINING PARAMETERS FOR BRUSH...
Journal Articles
Alloy Digest (1993) 42 (1): Cu-581.
Published: 01 January 1993
... 1-3 C3843 Table 2 - MELTING AND POURING RANGES Solidus Liquidus Pouring Range OF C F C OF C - - - - Brush Alloys 20C and 2m 1600 870 1780 970 1850-2050 1010-1120 Heat Treatments: The strength, hardness and elongation of Brush Ahoy 20C and 2OCf is achieved through age-hardening. The recommended...
Journal Articles
Alloy Digest (1992) 41 (9): Cu-576.
Published: 01 September 1992
... & Aged 135-145 930-1000 145-155 1000-1070 2-4 c34-39 Table 2 - MELTING AND POURING RANGES Solidus Liquidus F C F C Brush Alloys 165C and 165CT 1625 885 1810 990 Pouring Range F C 1850-2050 1010-l 120 DOI: 10.31399/asm.ad.cu0576 Copyright © ASM International® 1996 Table 3 -RECOMMENDED MACHINING...
Journal Articles
Alloy Digest (1992) 41 (12): Cu-537.
Published: 01 December 1992
... Solution Annealed & Aged 165-180 1140-1240 180-195 1240-1340 0.5-3 c43-47 Table 2 - MELTING AND POURING RANGES Solidus Liquidus Pouring Range F C F C F C Brush Alloys 275C and 275CT 1570 850 1710 930 1760-1900 960-1040 Heat Treatment: The. strength, hardness and elongation of Brush Alloys 275C and...