1-20 of 22 Search Results for

BRUSH ALLOY 165

Sort by
Journal Articles
Alloy Digest (1987) 36 (12): Cu-532.
Published: 01 December 1987
... BRUSH Alloy 165 has slightly less yield and fatigue strengths than the somewhat higher beryllium-content copper-beryllium alloy. It is cheaper and may be substituted when design requirements are less demanding. It is easily worked to provide complex shapes. This datasheet provides information...
Journal Articles
Alloy Digest (2014) 63 (6): Cu-832.
Published: 01 June 2014
... strength. It also includes information on forming. Filing Code: Cu-832. Producer or source: Materion Brush Performance Alloys. Producer or Source: Materion Brush Performance Alloys Copyright © ASM International® 2014 2014 ASM International bend strength BrushForm 158 chemical composition...
Journal Articles
Alloy Digest (1978) 27 (6): Cu-356.
Published: 01 June 1978
... BRUSH Alloy 25 attains the highest strength and hardness of any copper-base alloy. In the age-hardened condition, its tensile strength can exceed 200,000 psi and its Rockwell C hardness can reach 45. Its many applications include springs, deep-drawing parts, current-carrying springs connectors...
Journal Articles
Alloy Digest (1992) 41 (10): Cu-577.
Published: 01 October 1992
... BRUSH CASTING ALLOYS 245C AND 245CT are beryllium copper (2.25-2.55% Be) alloys of high strength with cobalt as the second alloying element (0.35-0.70% Co). Use is in the age-hardened temper. Brush casting alloy 245CT is the fine-grained version. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1970) 19 (6): Cu-217.
Published: 01 June 1970
... BRUSH alloy M25 is a free-machining beryllium-copper alloy having good response to age-hardening for high strength, hardness, fatigue and corrosion resistance. It is recommended for screw machine products, gears, shafts, hardware, fasteners, connectors, electronic and electrical components...
Journal Articles
Alloy Digest (1992) 41 (12): Cu-537.
Published: 01 December 1992
... Solution Annealed & Aged 165-180 1140-1240 180-195 1240-1340 0.5-3 c43-47 Table 2 - MELTING AND POURING RANGES Solidus Liquidus Pouring Range F C F C F C Brush Alloys 275C and 275CT 1570 850 1710 930 1760-1900 960-1040 Heat Treatment: The. strength, hardness and elongation of Brush Alloys 275C...
Journal Articles
Alloy Digest (1983) 32 (3): Cu-454.
Published: 01 March 1983
... BRUSH Alloy 3 offers the highest electrical and thermal conductivity of any beryllium-copper alloy. It possesses an excellent combination of moderate strength, good corrosion resistance and good resistance to moderately elevated temperatures. Because of its unique physical and mechanical...
Journal Articles
Alloy Digest (1998) 47 (11): Cu-624.
Published: 01 November 1998
... of Mechanical and Bending Properties C1741cqb) C17410@) wFsf4085 Brush 171 (Cl7450 -4085 CxTm) c70.?3c) wRM4cls5 c103-6(c) cTm(c) 556-6s 8&100 10-10 689-M lo&120 7-17 67L5-689 90-100 4-8 556-689 8&1co llmin 584-660 84-95 6-12 472 68 4 452-625 61-90 lOti 471-556 68-80 S-16 511 75 15 591-7& 85-110 7m 0.5 1.2 IO...
Journal Articles
Alloy Digest (1966) 15 (6): Cu-165.
Published: 01 June 1966
..., swirch jaws and blades, tapper roller bearings, flappe; valves, etc. Manufacturer: Anaconda American Brass Company, Waterbury, Connecticut Beryllium Corporation, Reading, Pennsylvania Brush Beryllium Corporation, Cleveland, Ohio (Also ocher copper alloy mills) Thv graph depicts the Sate design st 3s cuwe...
Journal Articles
Alloy Digest (1996) 45 (12): SS-664.
Published: 01 December 1996
... strip, cut sheets, round blanks, shapedblanks. Surfacefinish: IlIa/IIIc/IIId/lV/brushed. Specification Equivalents: Edge finish: Cut edges, rounded edges on request. Surface finishes: IIIa. heat neated. mechanicaUv &scaled. work hardened; IIIc, mechanically or chemically de&led. cold rolled. heat...
Journal Articles
Alloy Digest (1968) 17 (8): Cu-190.
Published: 01 August 1968
... HN) , mill hardened from 2 No. Hard (1. 2 Hb!) or mill hardened from 4 No. Hard (HM). Applications: Electrical contacts? springs, diaphrams. fuse clips, flapper valves, mechanical parts. Manufacturer: Practically all Be-Cu alloy manufacturers and Beryllium Corp., Reading. Pennsylvania and Brush...
Journal Articles
Alloy Digest (1997) 46 (8): SS-692.
Published: 01 August 1997
... rolled heat treated, pickled, and lightly rerolled) IIId(mechanicallyorchemkahydesc&d, cold ldkdhightarmealedandlightlYrerdled IV (ground) Brushed Edge Finish Cut edges, rounded edges on request (a) REMANIT 4436 can be mirror-polished. Sizes and thicknesses are as follows: Weldability: Remanit 4436...
Journal Articles
Alloy Digest (1984) 33 (11): Ni-305.
Published: 01 November 1984
... be applied by swabbing or brushing, or, if the parts are easily handled, by dipping. Additional information on preparing surfaces for welding is given in Huntington Alloys: Joining. Corrosion Resistance: The weld metal deposited from INCO-WELD A Electrode has an excellent resistance to corrosion...
Journal Articles
Alloy Digest (1996) 45 (8): SS-651.
Published: 01 August 1996
.... shaped blanks. 20.40 1000 1000 3ooo xm 1250 1250 4ooo >1.00-6.00 1524 1524 13.000 >713 1524 1524 6am surface finish: III al III cm cl/brushed Edge finish: Cut edges. rounded edges on request Applications: Due to its good corrosion resistance. cold workability. and weld- ability, Remanit 43 18 is widely...
Journal Articles
Alloy Digest (1997) 46 (10): SS-698.
Published: 01 October 1997
..., aluminum, and babbin Remail 4404 is resistant to inrergranular corrosion under con- tinuous opemting conditions at empedum to4OOTduetoits very low carbon content Products Available: Cold-rolled wide suip, split strip, cut sheets, round blanks, shaped blanks. Surface6nish:IIIa/IIIc/lIId/lV/brushed Edge...
Journal Articles
Alloy Digest (1984) 33 (7): Ni-300.
Published: 01 July 1984
... solutions are effective in cleaning before welding. The solutions may be applied by swabbing or brushing. or. if the parts are easily handled, by dipping. Additional tnformation on preparing surfaces ior welding is gnen in Huntington Alloys. Joining. Welding electrodes of 3 32. I 8. 5 32 and 3 l&inch...
Journal Articles
Alloy Digest (1984) 33 (9): Ni-302.
Published: 01 September 1984
.... This prevents embrittlement by corrosion products at welding temperatures. Cleaning can be done mechanically by grinding or machining, or chemically by pickling. Flash-pickling solutions are effective in cleaning before welding. The solutions may be applied by swabbing or brushing, or, if the parts are easily...
Journal Articles
Alloy Digest (2021) 70 (6): Cu-82.
Published: 01 June 2021
... 3 Fabrication characteristics Electrical chemical, textile and papermaking industries Mechanical Heavy-duty springs, clips and switch components. Characteristic or process Rating Capacity for being hot formed Poor Heavy-duty springs; diaphragms; wire brushes; Capacity for being cold formed Excellent...
Journal Articles
Alloy Digest (1985) 34 (10): Ni-323.
Published: 01 October 1985
... by swabbing or brushing, or, if the parts are easily handled, by dipping. Additional information on preparing surfaces for welding is given in Huntington Alloys: Joining. Corrosion Resistance: The weld metal deposited from welding Electrode 132 has good resistance to high-temperatue oxidation. Specification...
Journal Articles
Alloy Digest (1985) 34 (11): Ni-325.
Published: 01 November 1985
.... This prevents embrittlement by corrosion products at welding temperatures. Cleaning can be done mechanically by grinding or machining, or chemically by pickling. Flash-pickling solutions are effective in cleaning before welding. The solutions may be applied by swabbing or brushing. or. if the parts are easily...