Alloy Digest (1988) 37 (9): Ni-362.
Published: 01 September 1988
... BRIGHTRAY Alloy B is an electrical resistance wire which contains rare-earth long-life additions. It is useful up to 1100 C (2010 F). It has a greater temperature coefficient of resistance than the essentially binary 80/20 nickel chromium resistance grade. It is suitable for less exacting...
Journal Articles
Alloy Digest (1988) 37 (8): Fe-85.
Published: 01 August 1988
... Table 4 -- MULTIPLJERS FOR RESISTANCE CHANGE WITH TEMPERATURE (SLOWLY COOLED MATERIAL) Tempcranne. Oc 1093 982 871 760 640 538 482 427 316 204 93 Multiplier 23.5 22.5 21.4 19.6 17.8 15.6 14.4 13.0 10.0 6.5 2.6 Specification Equivalents B. S. S. 115 ASTMB344 General Characteristics BRIGHTRAY Alloy 35 has...