Alloy Digest (1988) 37 (8): Fe-85.
Published: 01 August 1988
... BRIGHTRAY Alloy 35 is an iron-nickel-chromium alloy containing long-life rare-earth additions. It is suitable for applications subject to frequent switching and wide temperature fluctuations to a maximum operating temperature of 1050 C(1920 F). It has a relatively large temperature coefficient of...
Journal Articles
Alloy Digest (1988) 37 (9): Ni-362.
Published: 01 September 1988
... 1.45 (0.0571 ) 0.666 (0.203 ) 20 0.8 13 (0.0320) 2.12 (0.646 ) 25 0.457 (0.0179) 6.71 (2.04 ) 30 0.254 (0.0100 ) 21.7 (6.62 ) 35 0.143 (0.0056) 68.5 (20.9 ) *For more complete design data contact producer. Length/weight meter/kg (ft/lb) 5.74 ( 8.54) 9.15 ( 13.6) 14.5 ( 21.6) 23.0 ( 34.3) 73.5 ( 109...
Journal Articles
Alloy Digest (2003) 52 (3): Ni-603.
Published: 01 March 2003
... 700 typical 102 typical 410 typical 59 typical 36 typical 35 typical 80 typical 59 typical 205 typical DOI: 10.31399/asm.ad.ni0603 resistance to hot cracking, tolerance to dilution by many combi- nations of nickel-base and ferrous alloys, and stable properties over a wide range of service...