Alloy Digest (1967) 16 (10): SA-217.
Published: 01 October 1967
... ATLAS BRAKE DIE is an electric furnace alloy steel specifically designed to provide the optimum balance of strength, wear resistance and toughness desired in brake-die applications. It is normally furnished in the heat treated and stress-relieved condition. This datasheet provides information...
Journal Articles
Alloy Digest (1976) 25 (6): TS-302.
Published: 01 June 1976
... BRAKE DIE is a medium-alloy tool steel heat treated at the mill by oil-quenching and tempering to develop the best combination of properties. It is used for all types of dies on hand-operated and mechanically operated press brakes for the forming and bending of sheets, strip and other flat-rolled...
Journal Articles
Alloy Digest (1970) 19 (9): Al-199.
Published: 01 September 1970
... ALUMINUM 392.0 is a hypereutectic aluminum-silicon alloy developed for die castings which require high resistance to wear and abrasion. Applications include variable speed pulleys, automotive clutch friction rings, cylinder liners, sheaves, and brake drums. This datasheet provides information...
Journal Articles
Alloy Digest (1973) 22 (10): TS-263.
Published: 01 October 1973
... BOFORS BP20-2 is a vacuum-degassed (BOVAC) alloy tool steel recommended for plastic molds, brake dies, die-casting dies for tin, lead and zinc alloys, and for constructional parts. It is supplied prehardened to 270-300 Brinell and needs no further heat treatment before use; however, it may be heat...
Journal Articles
Alloy Digest (1953) 2 (11): CI-4.
Published: 01 November 1953
... resistance as well as casting, heat treating, machining, and joining. Filing Code: CI-4. Producer or source: American Brake Shoe Company. Producer or Source: American Brake Shoe Company Copyright ┬ę ASM International┬« 1996 1996 ASM International ABK Metal chemical composition compressive...
Journal Articles
Alloy Digest (1997) 46 (12): SS-703.
Published: 01 December 1997
... Balance General Characteristics: 42OMB is a free machining mold base steel for plastic molds, die casting dies. mold bases, plates, and brake dies. The addition of molybdenum improves the corrosion resistance of 420MB versus AISI 420F. This may reduce or eliminate the need to chromium or electroless...
Journal Articles
Alloy Digest (2009) 58 (9): TS-683.
Published: 01 September 2009
... itself in abrasive applications, such as compression molding or mold injection when glass reinforced resin is required. Finkl HB Holder steel is for plastic molds, rubber molds, die casting dies, mold bases, plates, and brake dies. Finkl Hi-Hard P-20 is recommended for plastic molds, zinc die casting...
Journal Articles
Alloy Digest (2017) 66 (10): SA-801.
Published: 01 October 2017
... ArcelorMittal MTD 4 is a 4150 plate steel for applications such as press brake dies, machinery parts and short-run tools and dies where abrasion is a concern. This datasheet provides information on composition. It also includes information on forming, heat treating, machining, and joining. Filing...
Journal Articles
Alloy Digest (1957) 6 (2): Ti-11.
Published: 01 February 1957
... grinding ratio. For precision and internal grinding use low wheel speeds, somewhat below 1800 sfpm, with work speeds of 40 sfpm and feeds of 0.002 . Shearing, sawing, nibbling,. die blanking are all satisfactory methods of blank preparauon prior to formin . Gauges UP to .187 in thickness may be sheared...
Journal Articles
Alloy Digest (1953) 2 (10): Al-9.
Published: 01 October 1953
... ALUMINUM 218 is an aluminum die casting alloy having excellent combination of high strength and corrosion resistance, also high ductility and finishing qualities. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well...
Journal Articles
Alloy Digest (1957) 6 (8): Al-54.
Published: 01 August 1957
... APEX 418 is an aluminum die casting alloy having excellent combination of high strength and corrosion resistance, also high ductility and finishing qualities. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...
Journal Articles
Alloy Digest (1974) 23 (8): SA-307.
Published: 01 August 1974
... competitive products in equi- valent BrineU ranges) of the as-rolled product. A minimum die opening of 10T is recommended on the bottom or female die for press brake forming. Hot Forming of Plates: Occasionally it is found necessary to make severe bending formation that may be impossible to perform...
Journal Articles
Alloy Digest (1997) 46 (1): SA-484.
Published: 01 January 1997
... Lukens MTD steels are prehardened alloy plate steels developed for mold, tool, and die applications. This datasheet provides information on composition and hardness. It also includes information on heat treating, machining, and joining. Filing Code: SA-484. Producer or source: Lukens Steel Company...
Journal Articles
Alloy Digest (1996) 45 (10): SS-657.
Published: 01 October 1996
...: Remanit 4021 is used for parts prone to wear. for example, cutting blades. surgical instruments. die sheets, and brake discs. Producer: Thyssen Stahl AG Krefeld, Germany (02151) 83-01 In USA: Thyssen Specialty Steels, Inc. Carol stream, IL 60188 (708) 682-3900 SS-657B ...
Journal Articles
Alloy Digest (1960) 9 (1): SA-93.
Published: 01 January 1960
... Available: Forging billets, forgings either annealed or heat treated. Applications: Die casting dies, plastic moldst press brake dies, forge hammer rams, crankshafts, tong jaws, gears, shafting, axles and sprockets. Manufacturer: Vanadium Alloys Steel Company Latrobe, Pennsylvania ...
Journal Articles
Alloy Digest (1997) 46 (1): SS-669.
Published: 01 January 1997
... Applications: Producer: Cutlery, kitchen knives, pocket knife blades. meat knives, vemia callipm. surgical instruments, brake discs, and die sheets. Tbyssen StabI AG Krefeld. Germany (02151) 83-01 ISSN: 002-614X In USA: Thyssen specialty steels. Inc. carol strtam. IL 60188 (708) 682-3900 SS-669B ...
Journal Articles
Alloy Digest (1976) 25 (12): Cu-323.
Published: 01 December 1976
... - TYPICAL MECHANICAL PROPERTIES 0.31 8.5 1610-1630 0.09 11.5 x 10-6 18 16 x 106 6 x 106 Property Tensile strength, psi Yield strength (0.2% offset), psi Elongation (2 in % Brinell hardness (500-kg load) Sand Cast 53000 22000 23 80 Die Cast 63000 44000 7 110 Heat Treatment: DZR Yellow Brass is generally used...
Journal Articles
Alloy Digest (1968) 17 (2): SA-222.
Published: 01 February 1968
... for hoc die applications aold is an errablishcd srccl ior disc and drum rype aiccrafr brakes in large high speed l ircrafr. Thir grade is a high-strmgth, low-alloy sccel which has received vidc -spread ;pplicacion in scesm and gas turbine bolting up 10 nbouc 105oDF. 11 hns also kco used for various chrcr...
Journal Articles
Alloy Digest (1965) 14 (8): CS-23.
Published: 01 August 1965
... is required. some re*uct1on I" speeds may be required to benefit tool life and the use of a coolant is remmended for some machining operations. INX-Steels can be satisfactorily wc,rked on a draw bench, press brake, or other equipment used for cold i'rrci"S operations. me to their higher yield strengths...
Journal Articles
Alloy Digest (1960) 9 (2): Al-89.
Published: 01 February 1960
... Temperature Tensile Elongation Table 2 - TYPICAL CHILL CAST PROPERTIES AsCast T5 T7 Tensile strength, psi 25000 32OOO 38000 Elongation, $% in 2 o-l o-l o-1 BrineIl hardness (500/10) 85 loo 110 Table 3 - TYPICAL DIE CAST PROPERTIES T7 Tensile strength, psi Elongation, % in 2 Brinell hardness (5OO/lO) As Cast...