Skip Nav Destination
Close Modal
Search Results for
BR-4 DIE STEEL
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 26 Search Results for
BR-4 DIE STEEL
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1986) 35 (7): TS-460.
Published: 01 July 1986
... BR-4 is a high-carbon high-chromium die steel with unexcelled abrasive-resisting qualities. It has important secondary hardening properties. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information...
Abstract
View article
PDF
BR-4 is a high-carbon high-chromium die steel with unexcelled abrasive-resisting qualities. It has important secondary hardening properties. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-460. Producer or source: Latrobe Steel Company.
Journal Articles
Alloy Digest (1952) 1 (1): TS-1.
Published: 01 September 1952
... Latrobe BR-4 is a high-vanadium, high-chromium tool and die steel of the air hardening and nondeforming type. In the hardened condition it is extremely abrasion resistant. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information...
Abstract
View article
PDF
Latrobe BR-4 is a high-vanadium, high-chromium tool and die steel of the air hardening and nondeforming type. In the hardened condition it is extremely abrasion resistant. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information on heat treating, machining, and joining. Filing Code: TS-1. Producer or source: Latrobe Steel Company.
Journal Articles
Alloy Digest (1960) 9 (2): TS-90.
Published: 01 February 1960
... JET FORGE is a hot work die steel for forging high temperature alloys. It offers toughness and high wear resistance on high temperature applications involved in forging jet parts. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness...
Abstract
View article
PDF
JET FORGE is a hot work die steel for forging high temperature alloys. It offers toughness and high wear resistance on high temperature applications involved in forging jet parts. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-90. Producer or source: Vanadium Alloys Steel Company.
Journal Articles
Alloy Digest (1955) 4 (5): TS-33.
Published: 01 May 1955
... JESSOP 2-B machinability workability Filing Code: TS-33 JESSOP 2=B Tool Steel MAY 1955 - DATA ON WORLD WIDE METALS AND ALLOYS Pnblisbd br Engineering Alloys Di.mr. Irk. Upper Montclair. New Jrrscv JESSOP 2-B (Hot Work Die Steel) JESSOP 2-B is a general purpose hoc work die steel having great...
Abstract
View article
PDF
JESSOP 2-B is a general purpose hot work die steel having great resistance to abrasion. It is supplied in three grades. namely 2-B (L.C.), 2-B (M.C.) and 2-B (H.C.). These are classed as ASM Type IV F1, Type IV F3 and Type IV F2 respectively. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, and machining. Filing Code: TS-33. Producer or source: Jessop Steel Company.
Journal Articles
Alloy Digest (1966) 15 (12): TS-187.
Published: 01 December 1966
... Heppenstall Gr. 5M21 is a low-carbon, high-molybdenum and nickel precipitation hardening die steel developed especially for hot working of ferrous and nonferrous metals in press and upsetting machines. It is furnished to the Die Steel trade under the trade name of Prestem (in the prehardened...
Abstract
View article
PDF
Heppenstall Gr. 5M21 is a low-carbon, high-molybdenum and nickel precipitation hardening die steel developed especially for hot working of ferrous and nonferrous metals in press and upsetting machines. It is furnished to the Die Steel trade under the trade name of Prestem (in the prehardened condition) and Presneal (in the annealed condition). This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-187. Producer or source: Midvale-Heppenstall Company.
Journal Articles
Alloy Digest (1958) 7 (11): TS-76.
Published: 01 November 1958
... ATHA PNEU chemical composition die steel fracture toughness hardness heat treatability machinability tensile properties wear resistance workability I Filing Code: W-76 II ATHA PNEU Tool steel NOVEMBER 1958 Inn- DIGEST -DATA ON WORLD WIDE METALS AND ALLOYS- Publirbad br - -I Engineering...
Abstract
View article
PDF
ATHA PNEU is a shock resistant tool and die steel designed for applications requiring extreme toughness combined with good wear resistance and cutting properties. It conforms to AISI Type S1, SAE Type S1 and ASM Class III-D. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-76. Producer or source: Crucible Steel Company of America.
Journal Articles
Alloy Digest (1987) 36 (9): TS-481.
Published: 01 September 1987
... Characteristics: AL Tech Huron is a high-hardenability (Fignre I) nondeforming, high-carbon, high-chromium. cold-work tool and die steel combining high hardness and high compressive strength (Table 4) with exaUent wear qualities. It is recommended for long-run cold forming dies and similar applications where...
Abstract
View article
PDF
AL TECH HURON is a cold-work tool steel developed for applications requiring high resistance to wear or to abrasion and for resistance to heavy pressure rather than to sudden shock. Because of these qualities and its good nondeforming properties, it is unsurpassed (for an oil-hardening tool steel) for die work on long production runs. It has superior depth of hardening. Its many applications include cold trimmer dies, lamination dies, plug gages, slitting cutters and blanking, stamping and cold-forming dies and punches for long runs. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-481. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Alloy Digest (1968) 17 (8): TS-209.
Published: 01 August 1968
... Thermold-H10 is a chromium-molybdenum hot work steel that exhibits excellent resistance to softening at elevated temperatures. It is recommended for hot punches and shears, mandrels, and aluminum die casting dies. This datasheet provides information on composition, physical properties, hardness...
Abstract
View article
PDF
Thermold-H10 is a chromium-molybdenum hot work steel that exhibits excellent resistance to softening at elevated temperatures. It is recommended for hot punches and shears, mandrels, and aluminum die casting dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-209. Producer or source: Cyclops Corporation.
Journal Articles
Alloy Digest (1958) 7 (2): TS-67.
Published: 01 February 1958
.... 12 12 25 30 22 47 22 so Machinability*: At 800°F. 18 34 62 60 Machinability rating is considered as 70% of that of a l.Oo/" carbon tool steel (annealed), and about 457" of B1112 Bes- semer screw stock. Single point turning tools of high speed steel should be ground to 16-18 deg side rake, 4-7 deg...
Abstract
View article
PDF
CHRO-MOW is a tough hot work steel which will harden from a relatively low temperature in air. It possesses a desirable combination of toughness and red-hardness. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-67. Producer or source: Crucible Steel Company of America.
Journal Articles
Alloy Digest (1993) 42 (6): SS-545.
Published: 01 June 1993
... steam metal reformers thermal properties MARKER G4848 Filing Code: ss-545 Stainless Steel - DIGEST- JUNE 1993 DATA ON WORLD WIDE METALS AND ALLOYS PuMshedbyc Alloy Die% Inc. /201-677-9161 27 Cdiikl SVW. Orange. NJ. 07050 / USA MARKER G4848 (High Temperature Cast Austenitic Stainless Steel) MARKER...
Abstract
View article
PDF
Märker G4848 is a cast austenitic stainless steel for use up to 1050 C (1922 F). Typical uses include petrochemical ethylene furnace tubes and steam metal reformers. This datasheet provides information on composition and physical properties. It also includes information on casting and joining. Filing Code: SS-545. Producer or source: Schmidt & Clemens GmbH.
Journal Articles
Alloy Digest (1987) 36 (11): TS-484.
Published: 01 November 1987
... METALS AND ALLOYS NOVEMBER 1887 0 copyright 1987. Alloy ISSN:OO2414X Dora shown we ryprcd for spcifmwron or fhal Di#en. Inc. Au ri@m not IO k used &sign reIm%d. hblukd by: Alloy Dipn. br 27 CadkId S~recs Oman. New Jerry 07050 (201) 677.9161 AL TECH* B-47 (Hot-Work Tool Steel; AISI Type H19) AL TECH B-47...
Abstract
View article
PDF
AL TECH B-47 is a chromium-tungsten-cobalt-vanadium steel with excellent resistance to shock and abrasion at elevated temperatures. Its good hot hardness enables it to handle many hot-work jobs without washing out or changing size. B-47 has very good mechanical properties at elevated temperatures where typical applications include extrusion dies for brass, hot-punch tools and forging-die inserts. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-484. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Alloy Digest (1956) 5 (2): TS-43.
Published: 01 February 1956
... composition dies elasticity hardness heat treatability impact strength machinability tensile properties workability C. Y. W. CHOICE Filing Code: TS-43 Tool steel FEBRUARY 1956 - DATA ON WORLD WIDE METALS AND ALLOYS Prcblirbd br Ewgineehg Alkvs Digest, hc Uppa Momhir, New Jcaey C. Y. W. CHOICE (Hot...
Abstract
View article
PDF
C. Y. W. CHOICE steel is a chromium hot work steel developed for applications where dies or tools are subjected to heavy pressure or impact while in contact with hot metal. It is an ASM Class IV A-2 tool steel. This datasheet provides information on composition, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: TS-43. Producer or source: Firth Sterling Corporation.
Journal Articles
Alloy Digest (1971) 20 (12): SA-270.
Published: 01 December 1971
... g-4-20 Smd-Al oy DECEMBER 1071 DIGEST a - DATA ON WORLD WIDE METALS AND ALLOYS . pauidaiby -tiDibar,ioc Upper Montclair, New Jm REPUBLIC HP 94-20 (Heat-Treated Alloy Steel; Consumable Electrode Vacuum Melted) REPUBLIC HP g-4-20 is designed especially for applications requiring optimum combinations...
Abstract
View article
PDF
REPUBLIC HP 9-4-20 is designed especially for applications requiring optimum combinations of relatively high yield strength and toughness with good weldability. This alloy is capable of providing 180,000 psi yield strength in combination with a Charpy V-notch value of 50 ft-lb at 75 F in plate thicknesses up to at least 4 inches. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-270. Producer or source: Republic Steel Corporation.
Journal Articles
Alloy Digest (1972) 21 (4): Ti-64.
Published: 01 April 1972
...~in. nose radius. Workability: The alloy can be finished forged at a temperature of 16500F. Open and closed die forgings can be produced with conventional forging practices. Can be cold formed by procedures used for stainless steels in the STA and DA conditions. Forming at moderately elevated temperatures...
Abstract
View article
PDF
Ti-6A1-2Sn-4Zr-6Mo is a high-strength titanium-base alloy having excellent properites in the intermediate temperature range. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-64. Producer or source: Titanium Metals Corporation of America.
Journal Articles
Alloy Digest (1956) 5 (4): SA-41.
Published: 01 April 1956
... properties workability Filing Code: SA-41 Steel-Alloy APRIL 1956 - DATA ON WORLD WIDE METALS AND ALLOYS Pnblisbed br Engineering AiIoys Digest, IX Upper Monrciair, New Jersey HI-STEEL (High-Strength Low-Alloy Steel) HI-STEEL is a high-strength iow-ailoy srruccurai steel having good resistance...
Abstract
View article
PDF
HI-STEEL is a high-strength low-alloy structural steel having good resistance to atmospheric corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive, shear, and bearing strength as well as fracture toughness and fatigue. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-41. Producer or source: Inland Steel Company.
Journal Articles
Alloy Digest (1994) 43 (12): Fe-108.
Published: 01 December 1994
... Drilling (M32 High-Speed Ste.el Drills) Feed, ipr Speed Nominal Hole Diameter, inches fpm l/16 l/8 l/4 1R 314 1 11n 2 - - - - - - - - - 80-85 0.001 0.003 0.005 0.010 0.013 0.016 0.020 0.025 Tapping Tap at 25-30 fpm using M-l, M-7 or M-10 high-speed steel taps. Die Threading (M-l, M-2, M-7, or M-10 High...
Abstract
View article
PDF
Carpenter Silicon Core Iron A-FM, melted to exacting chemical specifications and carefully process controlled to produce a fine-grained uniform quality magnetic core iron. This alloy exhibits improved machining characteristics over Silicon Core Iron A (Alloy Digest Fe-94, January 1991). This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining. Filing Code: FE-108. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1967) 16 (10): TS-198.
Published: 01 October 1967
... br En,gineecing Alloys Dig@, Inc. Upper Moatdak, New Jersey (High-Carbon High-Chromium Tool Steel, Type D3) HURON is an oil hardening high-carbon high-chromium die steel designed for cold work applications involging wear or abrasion. It is recommended for long run punch, blanking and stamping...
Abstract
View article
PDF
HURON is an oil hardening high-carbon high-chromium die steel designed for cold work applications involging wear or abrasion. It is recommended for long run punch, blanking and stamping requirements. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-198. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
Alloy Digest (1990) 39 (4): Fe-90.
Published: 01 April 1990
..., ipr Cut-off Tool Width, in. Form Tool width, in. Tool Tool fpn 1/16 l/8 l/4 l/2 1 1 l/2 2MakriaI HS Steel 70 0.001 0.0015 0.002 0.0015 0.001 0.001 O.ooO7 M-2 Carbide 250 0.003 0.0045 0.006 0.003 0.0025 0.0025 0.0015 c-6 MilIinlrJEnd Peripheral, 0.050 Depth of Cut High-Speed M-42 Took Carbide C-6...
Abstract
View article
PDF
Carpenter Silicon Core Iron "B" is melted in electric arc furnaces to exacting chemical specifications, and carefully controlled in rolling and annealing practices to produce a fine grained uniform quality magnetic core alloy. Silicon Core Iron "B" is not recommended for components which must be cold formed due to its high silicon content. This alloy was covered with 4 other silicon core irons in Fe-36, November, 1968. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining. Filing Code: Fe-90. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1956) 5 (5): Cu-38.
Published: 01 May 1956
...;de fiber Form 1 die 0.S dh.d Table 3 - FATIGUE TESTS T-per Tensile Spcngrh Endurance Saengrb Million cycles Hard (9.4% draft) Hard (11.5% draft) 2*cO 2iOOO % Tassion Test Table 4 - IMPACT TESTS (ac room cempemnre on 0.7 diamem annealed spec;menS) Yield screngtb. psi (0.5% at.) Tensile screngcb, pi...
Abstract
View article
PDF
TOBIN BRONZE-452 is a copper-zinc alloy containing 0.75% of tin, having high strength, toughness and resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: Cu-38. Producer or source: American Brass Company.
Journal Articles
Alloy Digest (1976) 25 (2): TS-296.
Published: 01 February 1976
... DIGESTa - DATA ON WORLD WIDE METALS AND ALLOYS prblirbrJ br. UHB ROLAND* (Hot-Work Tool Steal 1 UHB ROLAND is a chromium-molybdenum-cobalt-vanadium tool steel characterized by good resistance to thermal shock and thermal fatigue, good high-temperature strength, good wear resistance and good machinability...
Abstract
View article
PDF
UHB ROLAND is a chromium-molybdenum-cobalt-vanadium tool steel characterized by good resistance to thermal shock and thermal fatigue, good high-temperature strength, good wear resistance and good machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-296. Producer or source: Uddeholm Aktiebolag.