Alloy Digest (2008) 57 (12): TS-675.
Published: 01 December 2008
... Boehler (or Böhler) S290 Microclean is a high-speed steel made by powder metallurgy which impacts toughness and machinability. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating and powder metal forms. Filing Code...