... Bismuth-Lead 55-45 is a bismuth-base eutectic alloy that melts at 255 F. It furnishes scientists and engineers with an easily castable material that is ready for use as soon as it freezes. It can be recovered readily and recycled into new uses any number of times. Its many uses include non...
Journal Articles
Alloy Digest (2021) 70 (1): Al-472.
Published: 01 January 2021
... Atlas 2011 is a wrought, heat-treatable, aluminum-copper alloy (2xxx series) that also contains small amounts of bismuth and lead. Both bismuth and lead promote high-speed machining by causing the chips to fracture during machining and breaking away from the cutting tool. Atlas 2011 is used in...
Journal Articles
Alloy Digest (1988) 37 (7): SA-431.
Published: 01 July 1988
... INcut 200 is a premium free-machining steel containing no lead. Machinability is derived from added bismuth. The steel has excellent ductility and it can be welded and brazed readily. The absence of lead facilitates of machine shop scrap. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1986) 35 (5): Bi-39.
Published: 01 May 1986
... soon as it freezes. It can be recovered readily and recycled into new uses any number of times. Its many uses include non-shrinking patterns, proof-casting, sealing heat-treating furnaces and bending large tubes (diameter greater than 1% inches). Composition: Bismuth Lead Nominal 55 45 Physical...
Journal Articles
Alloy Digest (1997) 46 (3): Al-341.
Published: 01 March 1997
... 0.15 Balance m Li-sllu@ Yrldsaenoh w =d==P- MPa ki MFa ksi i2i+ ToOkk2011-I3 379 55 296 4%) 15 Toobite2o11-I.451 310 45 179 26 25 TOObilC~ll-l-3 407 59 310 45 12 (a)Siigrcamdran1XinwillhaveslighrlyIwr-sam@nrlUa. Table 2 Minimum Mechanical Properties m ulbate~ yisrrmslb - -d==F- MPa Ird MPa ti rn2ieZ...
Journal Articles
Alloy Digest (1988) 37 (5): Cu-538.
Published: 01 May 1988
... 0.0018 max. Selenium 0.0010 max. Tellurium 0.0010 max. Bismuth 0.0010 max. Lead 0.0010 max. Oxygen 0.0010 max. Phosphorus 0.0003 max. Cadmium 0.0001 max. Mercury 0.ooo1 max. Zinc 0.0001 max. *The total Se, Te, Bi, As, Sb, Sn and Mn must not exceed 0.0040%. Physical Constents: Density, lb/cu in. (At 68°F...
Journal Articles
Alloy Digest (1977) 26 (11): Bi-1.
Published: 01 November 1977
..., soldering and sealing. *ASARCOLO is a registered trademark of ASARCO Incorporated. - Composition: Physical Constants: ASARCOLO ASARCOLO 158 - 255 - Bismuth 50 55 Density, lb/cu in. Lead 26.7 45 Specific gravity (At 680F) Tin 13.3 - Melting point, oF Cadmium 10 - Specific heat (solid), Btu/lb/oF Latent heat...
Journal Articles
Alloy Digest (1990) 39 (11): Cu-554.
Published: 01 November 1990
... anneal resistance to the materials. Composition: Copper (including silver) 99.88 min. AlStXliC 0.012 max. Antimony 0.003 max. Tellurium + selenium 0.025 max. Nickel 0.050 max. Bismuth 0.003 max. Lead 0.004 max. Silver, minimum % * Cl2708 0.027 ( 8) Cl2800 0.034 (10) Cl2900 0.054 (16) Cl3000 0.085 (25...
Journal Articles
Alloy Digest (1974) 23 (5): Cu-278.
Published: 01 May 1974
... Deoxidants None Sulfur 0.0018 max. Selenium 0.0010 max. Tellurium 0.0010 max. Bismuth 0.0010 max. Lead 0.0010 max. Oxygen 0.0010 max. Phosphorus 0.0003 max. Cadmium 0.0001 max. Mercury 0.0001 max. Zinc 0.0001 max. Density, Ib/cu in. (At 680F) Specific gravity Melting point, oF (Solidus and Liquidus) Specific...
Journal Articles
Alloy Digest (2014) 63 (12): Cu-834.
Published: 01 December 2014
... C10100 AND C10200 (Pure Copper Alloys) ANSONIA ALLOY C10100 AND C10200 Chemical Composition, wt (Maximum ppm) C10100 Copper 99.99 min Antimony 4.0 Arsenic 5.0 Bismuth 1.0 Cadmium 1.0 Iron 10.0 Lead 5.0 Manganese 0.5 Nickel 10.0 Oxygen 5.0 Phosphorus 3.0 Selenium 3.0 Silver 25.0 Sulfur 15.0 Tellurium 2.0...
Journal Articles
Alloy Digest (2018) 67 (1): Al-456.
Published: 01 January 2018
... heat treatability Kaiser Alloy K211 physical properties shear strength tensile properties workability thermal properties Kaiser Alloy K211 is a rod and bar alloy RoHS compliant 2011. Chemical Composition, wt.% Silicon 0.40 max Iron 0.7 Copper 5.0 6.0 Lead 0.20 0.4 Bismuth 0.20 0.6 Zinc 0.30...
Journal Articles
Alloy Digest (1998) 47 (5): Al-348.
Published: 01 May 1998
... coating acceptance. See alsa4Uoy Digest AL282. Alcoa and Excalibar 6013 are registered trademarks of Alcoa. Chemical Composition, wt (Maximum unless shown as a range. contains a nominal level of 0.5% lead and bismuth) Silicon 0.6-1.0 Iron 0.5 Copper 0.60-1.10 Manganese 0.2-O-8 Magnesium 0.8-l .2 Chromium...
Journal Articles
Alloy Digest (1999) 48 (9): Al-361.
Published: 01 September 1999
... Titanium 0.15 max Lead 0.40 0.7 Bismuth 0.40 0.7 Others, each 0.05 max Others, total 0.15 max Aluminum bal Physical Properties: Density at 20 °C (68 °F), kg/m3 (lb/in.3) 2710 (0.098) Melting range, °C (°F) 582 652 (1078 1204) Coefficient of linear thermal expansion at 20 100 °C (68 212 °F), 10 6/K (10 6/°F...