Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (4): SA-842.
Published: 01 April 2019
... Bisalloy Structural 80 steel (80 ksi minimum yield strength) is a low-carbon, low-alloy, high-strength structural steel exhibiting excellent cold formability and low-temperature fracture toughness. This datasheet provides information on composition, physical properties, and tensile properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (5): SA-844.
Published: 01 May 2019
... Bisalloy Structural 80 Pressure Vessel Steel (80 ksi minimum yield strength) is a low-carbon, low-alloy, high-strength structural steel for pressure vessel applications. It exhibits excellent cold formability and low-temperature fracture toughness. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (2): SA-839.
Published: 01 February 2019
... Bisalloy Structural 60 steel (60 ksi minimum yield strength) is a low-carbon, low-alloy, high-strength structural steel exhibiting excellent cold formability and low-temperature fracture toughness. This datasheet provides information on composition and shear strength. It also includes information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (3): SA-840.
Published: 01 March 2019
... Bisalloy Structural 70 steel (70 ksi minimum yield strength) is a low-carbon, low-alloy, high-strength structural steel exhibiting excellent cold formability and low-temperature fracture toughness. This datasheet provides information on composition, physical properties, hardness, tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (6): Sa-846.
Published: 01 June 2019
.... It also includes information on forming and machining. Filing Code: SA-846. Producer or source: Bisalloy Steels Group Limited. Producer or Source: Bisalloy Steels Group Limited Copyright ┬ę ASM International┬« 2019 2019 ASM International BISALLOY STRUCTURAL 100 STEEL chemical composition...