Alloy Digest (2019) 68 (3): SA-840.
Published: 01 March 2019
... Bisalloy Structural 70 steel (70 ksi minimum yield strength) is a low-carbon, low-alloy, high-strength structural steel exhibiting excellent cold formability and low-temperature fracture toughness. This datasheet provides information on composition, physical properties, hardness, tensile...
Journal Articles
Alloy Digest (2019) 68 (5): SA-844.
Published: 01 May 2019
....) Specification 790 930 (115 135) Typical 830 (120) 70 100 mm (2.76 3.94 in.) Specification 720 900 (104 131) Elongation in 50 mm (2.0 in GL, % 6 65 mm (0.24 in.) Specification, min 18 Typical 26 70 100 mm (2.76 3.94 in.) Specification, min 16 Hardness, typical, HB 255 Fabricability This alloy has good cold...