Alloy Digest (2019) 68 (6): Sa-846.
Published: 01 June 2019
.... It also includes information on forming and machining. Filing Code: SA-846. Producer or source: Bisalloy Steels Group Limited. Producer or Source: Bisalloy Steels Group Limited Copyright © ASM International® 2019 2019 ASM International BISALLOY STRUCTURAL 100 STEEL chemical composition...
Journal Articles
Alloy Digest (2019) 68 (3): SA-840.
Published: 01 March 2019
... Bisalloy Structural 70 steel (70 ksi minimum yield strength) is a low-carbon, low-alloy, high-strength structural steel exhibiting excellent cold formability and low-temperature fracture toughness. This datasheet provides information on composition, physical properties, hardness, tensile...
Journal Articles
Alloy Digest (2019) 68 (4): SA-842.
Published: 01 April 2019
...) Typical 100 (74) Hardness, HB 255 Copyright © 2019, ASM International®. All rights reserved. BISALLOY STRUCTURAL 80 (Structural Steel) Filing Code: SA-842 Steel Alloy :: Arpil 2019 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.4634 :: www.asminternational.org :: MemberServiceCenter...
Journal Articles
Alloy Digest (2019) 68 (5): SA-844.
Published: 01 May 2019
... (lb/in.3) 7750 (0.280) Mechanical Properties 0.2% proof stress, MPa (ksi) Specification, min 690 (100) Typical 750 (109) Tensile strength, MPa (ksi) Copyright © 2019, ASM International®. All rights reserved. BISALLOY STRUCTURAL 80 PRESSURE VESSEL STEEL (Structural Steel) Filing Code: SA-844 Alloy...
Journal Articles
Alloy Digest (2019) 68 (2): SA-839.
Published: 01 February 2019
... Bisalloy Structural 60 steel (60 ksi minimum yield strength) is a low-carbon, low-alloy, high-strength structural steel exhibiting excellent cold formability and low-temperature fracture toughness. This datasheet provides information on composition and shear strength. It also includes information...