Alloy Digest (1982) 31 (7): SA-385.
Published: 01 July 1982
... BETHSTAR 80 steel plate is a high-strength product with an 80,000 psi minimum yield strength. It attains this strength in the as-rolled condition through the combination of a low-carbon microalloyed chemistry and controlled (proprietary) processing. It offers substantial cost savings when compared...
Journal Articles
Alloy Digest (2003) 52 (9): SA-520.
Published: 01 September 2003
.... Extremely severe forming should be done hot, after heating the plate to a maximum of 593 °C (1100 °F). Weldability: BethStar grades 50, 60, 70, and 80 are readily weldable using conven- tional arc welding processes. Specified base metal strength and toughness can be maintained into the weld zone, provided...