Alloy Digest (1986) 35 (8): SA-421.
Published: 01 August 1986
... BethStar 60 steel plate is a high-strength product with a 60,000 psi minimum yield strength. It contains low carbon and low sulfur and has outstanding toughness, weldability and formability. It provides the design engineer with a an economical high-strength low-alloy (HSLA) grade that can...
Journal Articles
Alloy Digest (2003) 52 (9): SA-520.
Published: 01 September 2003
.... Extremely severe forming should be done hot, after heating the plate to a maximum of 593 °C (1100 °F). Weldability: BethStar grades 50, 60, 70, and 80 are readily weldable using conven- tional arc welding processes. Specified base metal strength and toughness can be maintained into the weld zone, provided...