Alloy Digest (1978) 27 (4): TS-332.
Published: 01 April 1978
... BETHLEHEM M-7 is a high-molybdenum type of high-speed steel. Because of its high-carbon and high-vanadium contents, it has superior resistance to abrasion and is used for tools where edge toughness and wear resistance are required. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1977) 26 (6): TS-319.
Published: 01 June 1977
... BETHLEHEM M-2 is a molybdenum-tungsten type of high-speed steel. In general, it can be used for the same applications as the 18 tungsten-4 chromium-1 vanadium (AISI Type T1) high-speed steel. Its higher carbon content (relative to Type T1) and balanced composition produce properties applicable...
Journal Articles
Alloy Digest (1961) 10 (4): TS-104.
Published: 01 April 1961
... machinability wear resistance workability All BETHLEHEM 57 SPECIAL Filing Code: TS-104 Tool Steel APRIL 1961 P&M by Eagioeeting Alloys D&e& Inc. BETHLEHEM 57 SPECIAL (Hot-Work Tool Steel, Type H25) Upper Martdsir, New Jasev BETHLEHEM 57 SPECIAL is the 14% tungsten type of hot-work tool steel. It has high...
Journal Articles
Alloy Digest (1989) 38 (8): CS-125.
Published: 01 August 1989
...-7116 36-138 to 600 7/16-l l/4 36-150 to 600 Applications: Machinery designed for cold-weather use, shipbuilding, offshore drill rigs. Producer: Bethlehem Steel Corporation Bethlehem, Pennsylvania 18016 ...
Journal Articles
Alloy Digest (1959) 8 (8): TS-84.
Published: 01 August 1959
... Cooled Brineil T&pera&e Fracture Rockwell Brinell Fracture Rockwell OF. Rating C Hardness Rating c 1900 7% 2; 444 5% 2000 8% 477 $ 2100 8% 51 495 $2 50 2150 514 20 ii 5 : 78 s 5 2 2250 7% 30 5 2: iii: 7% 5 2 Table 2 -RFFFCT OF TEMPERING TEWPRRATURE (Specimens 1 in round by 1 M in. long were hardened...
Journal Articles
Alloy Digest (1972) 21 (3): SA-272.
Published: 01 March 1972
... BETHLEHEM RQ-100A is a heat-treated alloy steel having 100,000 psi yield strength through 11/4-in. thickness, in combination with good toughness, abrasion resistance and weldability. It is engineered specifically for structural applications such as earth moving equipment,buildings, bridges...
Journal Articles
Alloy Digest (1972) 21 (12): TS-248.
Published: 01 December 1972
... BETHLEHEM HW 8 is a high-alloy hot-work tool steel containing chromium, molybdenum and vanadium. Its combined characteristics comprise high red-hardness, high abrasion-resistance, resistance to heat-checking, and adequate toughness for its many applications. This datasheet provides information...
Journal Articles
Alloy Digest (1957) 6 (4): TS-57.
Published: 01 April 1957
... BETHLEHEM Cr-Mo-W is a general purpose hot work tool and die steel having excellent resistance to wear, shock, and drastic changes in temperature. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1974) 23 (4): TS-270.
Published: 01 April 1974
.../oF (70-2000F) 0.28 (704OOoF) 18.00 (7@8OOoF) 4.00 (70-l 2000F) 1.10 (70-l 5000F) Remainder Modulus of elasticity, psi PROPERTIES Table 1 - EFFECT OF QUENCHING TEMPERATURE ON HARDNESS (Specimens l-in. dia by 5-m long were austenitized, quenched as indicated and used for grain size and hardness) Quenching...
Journal Articles
Alloy Digest (1956) 5 (7): TS-48.
Published: 01 July 1956
... BETHLEHEM 67 CHISEL is the general-purpose, tungsten-type of shock-resisting tool steel. It has excellent properties for cold battering tools and hot-work shock applications. It is characterized by unusual toughness, resistance to fatigue and relative ease of heat treatment. This datasheet...
Journal Articles
Alloy Digest (1967) 16 (8): TS-196.
Published: 01 August 1967
... toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-196. Producer or source: Bethlehem Steel Corporation. Producer or Source: Bethlehem Steel Corporation Copyright © ASM International® 1996 1996 ASM International A-H5 chemical composition...
Journal Articles
Alloy Digest (1952) 1 (3): TS-3.
Published: 01 November 1952
... BETHLEHEM HOT WORK 8 alloy is a hot-work tool steel having high wear resistance in the higher range of operating temperatures. It also has high resistance to surface wash and heat-checking. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1977) 26 (2): TS-313.
Published: 01 February 1977
... information on composition and hardness as well as fracture toughness. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-313. Producer or source: Bethlehem Steel Corporation. Producer or Source: Bethlehem Steel Corporation Copyright © ASM...
Journal Articles
Alloy Digest (1967) 16 (6): SA-211.
Published: 01 June 1967
... FOR MAXIMUhl CASE HARDNESS (Specimens 0.565 dia., carburized 1700cF for 8 hours) (Single hear resulrs - 0.22C-Bethlehem) Direct Quench Single Quench Double Quench from Poe-(A1 & Temper-(B) & Temper-(C) Tensile strength, psi 205500 191500 142250 Yield point, psi 168500 170250 81250 Elongation, 7. in 2 14.5...
Journal Articles
Alloy Digest (1958) 7 (11): SA-77.
Published: 01 November 1958
... - 180 1200 63-65 262 100% woody -310 Table 7 --MASS EFFECT DATA (Oil quenched from 1525 F. and tempered) fSingle heat results, 0.39C. .90 Mn. 0.46 Ni. 0.41 Cr. 0.10 MO) (Grain size 6-8 Bethlehem) Tensile Yield DiiZ Strength Point Elongation TiduE Brinell psi psi 70 in 2 % Hardness Tempered at 1000°F. Y...
Journal Articles
Alloy Digest (2001) 50 (1): SS-815.
Published: 01 January 2001
... and bend strength It also includes information on forming, heat treating, and joining. Filing Code: SS-815. Producer or source: Bethlehem Lukens Plate. Producer or Source: Bethlehem Lukens Plate Copyright © ASM International® 2001 2001 ASM International bend strength chemical composition...
Journal Articles
Alloy Digest (1975) 24 (3): Cu-293.
Published: 01 March 1975
... NJZ BRASCO is a powder metallurgy copper-zinc-cobalt alloy designed for use in the as-sintered condition. It provides sintered parts with substantially higher strength and hardness than conventional 70 copper/30 zinc brass P/M parts. Also, it undergoes significantly less dimensional change than 70...
Journal Articles
Alloy Digest (1957) 6 (11): SA-63.
Published: 01 November 1957
... distance l/l6 inch) ~ m~tance 48 1 45 2 42 3 39 4 34 5 31 6 7 12 29 27 8 23 21 16 R min 41 35 27 24 21 - - - - - Box quenched 1700°F. Reheated 142S°F., oil quenched and tempered 300°F. Box cooled, reheated 1575 F., oil quenched tempered 300°F. 0 -25 -65 Room 0 -25 -65 Room 0 -25 -65 Heat Treatment...
Journal Articles
Alloy Digest (1958) 7 (8): SA-73.
Published: 01 August 1958
...) (Bethlehem Single Heat Results, .58C, .78Mn, 2.OSi, .08Ni, .08Cr) Tempering Temperature OF. 400 ~~ 700 800 900 1000 1100 1200 1300 Tensile Strength DSi Diameter inches 305000 295000 280000 261000 233000 205000 181000 160000 144000 130000 Tensile Strength psi Yield Reduction Point Elongation of Area psi co...
Journal Articles
Alloy Digest (1959) 8 (6): SA-84.
Published: 01 June 1959
..., psi 2x00: 148000 Yield point. psi Elongation, % in 2 :; 10802 Reduction of area, % BrineU hardness 223 3:; kod imm ft. Ibs. 27 11 Table 2 - TYPICAL HEAT TREATED PROPERTIES-Single Heat Results* (0.530 Rd., normalized 1600°F.. reheated ro 1500°F.. oil quenched and tempered-Bethlehem) Tensile Yield...