Alloy Digest (1975) 24 (4): TS-286.
Published: 01 April 1975
... BETHLEHEM M-10 is a high-molybdenum type of high-speed steel. It is a general-purpose steel for cutting tools such as twist drills and is used for many other single- and multiple-point cutting applications. This datasheet provides information on composition, physical properties, and hardness as...
Journal Articles
Alloy Digest (1978) 27 (4): TS-332.
Published: 01 April 1978
... BETHLEHEM M-7 is a high-molybdenum type of high-speed steel. Because of its high-carbon and high-vanadium contents, it has superior resistance to abrasion and is used for tools where edge toughness and wear resistance are required. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1977) 26 (6): TS-319.
Published: 01 June 1977
... BETHLEHEM M-2 is a molybdenum-tungsten type of high-speed steel. In general, it can be used for the same applications as the 18 tungsten-4 chromium-1 vanadium (AISI Type T1) high-speed steel. Its higher carbon content (relative to Type T1) and balanced composition produce properties applicable to...
Journal Articles
Alloy Digest (1975) 24 (7): TS-289.
Published: 01 July 1975
... Bethlehem M-1 is a high-molybdenum, low-tungsten type of high-speed tool steel. It has good cutting ability except for heavy-duty, continuous cutting operations where the ultimate in red-hardness is required. This datasheet provides information on composition, physical properties, hardness, and...
Journal Articles
Alloy Digest (1979) 28 (9): CS-77.
Published: 01 September 1979
... higher finishing temperatures. **This is the approximate tensile strength and is listed for general information purposes. Bethlehem AR-235 is not furnished to a specific strength level. 0.284 7.85 0.11 6.7 x 10-6 7.0 x 10-6 7.4 x 10-6 28-30 x 106 12 x 106 Heat Treatment: Bethlehem AR-235 is supplied in...
Journal Articles
Alloy Digest (1974) 23 (4): TS-270.
Published: 01 April 1974
... BETHLEHEM T-1 is the 18 tungsten-4 chromium-1 vanadium high-speed steel and is used for general-purpose cutting operations. It has a balanced combination of shock-resistance and abrasion-resistance for cutting tools, high red-hardness and decarburizes the least of the standards high-speed steels...
Journal Articles
Alloy Digest (1956) 5 (7): TS-48.
Published: 01 July 1956
... Alto M Universal-Cyclops Par Exe Vanadium Alloys Q. A. Vulcan-Crucible General Characteristics: Bethlehem No. 67 Chisel steel is an oil-hardening tool steel. It has maximum shock-resistance for cold or hot-work appli- cations, bas good wear resistance and good red-hardness value. It is a versatile...
Journal Articles
Alloy Digest (1967) 16 (8): TS-196.
Published: 01 August 1967
... Molybdenum 1.10 200~800°F 7.19 Vanadium 0.25 200-1000°F 7.76 Chromium 5.25 200-12000F Iron Remainder Specific heat, Bm/lb./oF 7.91 g 0.113 m 0.119 68-1112°F 0.132 68-147 OF Modulus of elasticity, psi I 10 t 0-w 29.5 PROPERTIES Table 1 - TYPICAL ANNEALED PROPERTIES Tensile strength, psi 103000 Yield screngch...
Journal Articles
Alloy Digest (1972) 21 (3): SA-272.
Published: 01 March 1972
... BETHLEHEM RQ-100A is a heat-treated alloy steel having 100,000 psi yield strength through 11/4-in. thickness, in combination with good toughness, abrasion resistance and weldability. It is engineered specifically for structural applications such as earth moving equipment,buildings, bridges, and...
Journal Articles
Alloy Digest (1959) 8 (8): TS-84.
Published: 01 August 1959
... BETHLEHEM 57HW is the 9% tungsten type of hot-work tool steel, having excellent red-hardness and abrasion resistance compared with relatively good shock resistance for high operating temperatures. It corresponds to AISI Type H21 hot work tool steel. This datasheet provides information on...
Journal Articles
Alloy Digest (1974) 23 (6): TS-272.
Published: 01 June 1974
... lOOoF) Modulus of elasticity, psi PROPERTIES Table 1 - EFFECT OF QUENCHING TEMPERATURE ON HARDNESS (Specimens l-in. dia by 3-m. long were austenitized 1 hour at temperature, quenched as indicated and used for grain sire and hardness) 0.285 7.90 7.62x 10-6 2%30x 106 Quenching Air Quenched Oil Quenched...
Journal Articles
Alloy Digest (1989) 38 (8): CS-125.
Published: 01 August 1989
... BETHLEHEM RQ 100L is a low-carbon, low-sulfur, 100 ksi minimum yield strength quenched-and-tempered plate steel offering improved toughness and weldability over other quenched-and-tempered plate grades. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (2000) 49 (12): SA-506.
Published: 01 December 2000
... lighter superstructures and the use of shallower girders that may permit bridge designers to reuse the existing substructure elements. Product Forms Available: Lengths to 15.2 m (50 ft), widths to 4.95 m (195 in and thickness to 102 mm (4 in based on quenched and tempered material from Bethlehem Lukens...
Journal Articles
Alloy Digest (1992) 41 (1): SA-383.
Published: 01 January 1992
... BETHLEHEM HOT-ROLLED SHEET XF SERIES alloys B50XF, B60XF, B70XF and B80XF are high strength low alloy steels. The numbers in the alloy designations refer to minimum yield strengths. The steels are made using ladle desulfurization which virtually eliminates harmful stringer type inclusions. The...
Journal Articles
Alloy Digest (1957) 6 (4): TS-57.
Published: 01 April 1957
... BETHLEHEM Cr-Mo-W is a general purpose hot work tool and die steel having excellent resistance to wear, shock, and drastic changes in temperature. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on...
Journal Articles
Alloy Digest (1952) 1 (3): TS-3.
Published: 01 November 1952
... BETHLEHEM HOT WORK 8 alloy is a hot-work tool steel having high wear resistance in the higher range of operating temperatures. It also has high resistance to surface wash and heat-checking. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1954) 3 (10): TS-26.
Published: 01 October 1954
... compressive strength as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-26. Producer or source: Bethlehem Steel Corporation. Producer or Source: Bethlehem Steel Corporation Copyright © ASM International® 1996 1996 ASM International...
Journal Articles
Alloy Digest (1973) 22 (7): SA-291.
Published: 01 July 1973
... kJ/in. (24~. 160a, 11.5 in./min) CMA (A + 2% 0) 0.250 Linde 83 2 20 kJ/in. (27.5~. 280a, 23 in./mti) GhlA (A + 2% 0) 0.115 Linde 83 1 8 kJ/m. (19v. 140a, 20 in./min) Abbreviations: SMA = Shielded Metal .4rc. GMA = Gas Metal Arc. A = Argon 0 = Osygen 0.282 7.81 0.12 6.8 x 10-6 28-30 x 106 DOI...
Journal Articles
Alloy Digest (1969) 18 (12): TS-225.
Published: 01 December 1969
... on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-225. Producer or source: Bethlehem Steel Corporation. Producer or Source: Bethlehem Steel Corporation Copyright © ASM International...
Journal Articles
Alloy Digest (1976) 25 (6): TS-302.
Published: 01 June 1976
... information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-302. Producer or source: Bethlehem Steel Corporation. Producer or Source: Bethlehem Steel Corporation Copyright © ASM International® 1996 1996 ASM International BRAKE...