Alloy Digest (1952) 1 (3): TS-3.
Published: 01 November 1952
... BETHLEHEM HOT WORK 8 alloy is a hot-work tool steel having high wear resistance in the higher range of operating temperatures. It also has high resistance to surface wash and heat-checking. This datasheet provides information on composition, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1972) 21 (12): TS-248.
Published: 01 December 1972
... BETHLEHEM HW 8 is a high-alloy hot-work tool steel containing chromium, molybdenum and vanadium. Its combined characteristics comprise high red-hardness, high abrasion-resistance, resistance to heat-checking, and adequate toughness for its many applications. This datasheet provides information...
Journal Articles
Alloy Digest (1961) 10 (4): TS-104.
Published: 01 April 1961
... machinability wear resistance workability All BETHLEHEM 57 SPECIAL Filing Code: TS-104 Tool Steel APRIL 1961 P&M by Eagioeeting Alloys D&e& Inc. BETHLEHEM 57 SPECIAL (Hot-Work Tool Steel, Type H25) Upper Martdsir, New Jasev BETHLEHEM 57 SPECIAL is the 14% tungsten type of hot-work tool steel. It has high...
Journal Articles
Alloy Digest (1959) 8 (8): TS-84.
Published: 01 August 1959
... BETHLEHEM 57HW Tool Steel r AUGUST 1959 J - DATA ON WORLD WIDE METALS AND ALLOYS Psblisbd br Engineering Alloys l5h Inc. Upper bhdair, New Jersey BETHLEHEM 57HW (Tungsten Hot Work Tool Steel Type H21) BETHLEHEM 57HW is the 9% mngsten type of hot-work tool steeI, having excellent red-hardness and abrasion...
Journal Articles
Alloy Digest (1977) 26 (2): TS-313.
Published: 01 February 1977
... by (Hot-Work Tool Steel; AISI Type Hll) Engineering Alloys Digest, Inc. Upper Montclair, New Jersey CROMO-V is a 5% chromium hot-work steel with an excellent combination of red-hardness, shock resistance and abrasion re- sistance; these are the properties needed for good hot-work characteristics...
Journal Articles
Alloy Digest (1977) 26 (6): TS-319.
Published: 01 June 1977
..., hot-work and shock-resisting tools are usually tempered within a range of 1100 to 12000F. The effect of tempering Bethlehem M-2 at various temperatures is shown in Table 3. Decarburization: Proper furnace atmosphere with correct hold- ing time and temperature are necessary precautions to prevent...
Journal Articles
Alloy Digest (1968) 17 (10): TS-211.
Published: 01 October 1968
... to machine and heat treat. Forms Available: Bars, rods, and forgings. Applications: Trimmer dies, die-casting dies, bolt-gripper dies, hoc shear blades, punches, hot forging dies. bolt- heading dies, and various orher types of bot- working cools. Monufocturer: Bethlehem Steel Corporation Bethlehem...
Journal Articles
Alloy Digest (1956) 5 (7): TS-48.
Published: 01 July 1956
... Exe Vanadium Alloys Q. A. Vulcan-Crucible General Characteristics: Bethlehem No. 67 Chisel steel is an oil-hardening tool steel. It has maximum shock-resistance for cold or hot-work appli- cations, bas good wear resistance and good red-hardness value. It is a versatile steel with excellent properties...
Journal Articles
Alloy Digest (1957) 6 (4): TS-57.
Published: 01 April 1957
... BETHLEHEM Cr-Mo-W is a general purpose hot work tool and die steel having excellent resistance to wear, shock, and drastic changes in temperature. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1970) 19 (10): SA-257.
Published: 01 October 1970
... by the usual methods employed for structural carbon steel, with adjustment of practice to allow for their greater strength. They are readily hot-worked or hot-formed. Recommended practices for cold forming are given in Table 4 for structural products and in Table 5 for sheet and strip. Weldability: Bethlehem V...
Journal Articles
Alloy Digest (1974) 23 (4): TS-270.
Published: 01 April 1974
... is rated at 100, T-l is given a rating of 60. Workability: Bethlehem T-l can be hot worked readily. Preheat and soak at about 13000F before transferring to the high-temperature heating furnace. Heat T-l slowly to the forging range of 2050 to 21500F. Discontinue forging as soon as the piece has cooled...
Journal Articles
Alloy Digest (1974) 23 (6): TS-272.
Published: 01 June 1974
... 212 max, ART has a machin- ability rating of 65, as compared with a 1 pet carbon tool steel rated at 100. Workability: Bethlehem A-HT has good hot-working properties. In heating for forging, preheat to 12500F and soak thoroughly. Then raise to 2000 to 2050oF. and hold until the steel is uniformly...
Journal Articles
Alloy Digest (1973) 22 (2): TS-250.
Published: 01 February 1973
... Cromo-WV is a 5% chromium-tungsten-vanadium-molybdenum tool steel for all general-purpose hot-work tools and dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1964) 13 (1): TS-142.
Published: 01 January 1964
... heat treatability high-temperature alloys joinability machinability mandrels physical properties tensile properties workability workability dies Filing Cede: TS-142 Toal steel CROMO-N JANUARY 1964 -DATA ON WORLD WIDE METALS AND ALLOYS CROMO-N (Hot Work Die Steel) ~&bed...
Journal Articles
Alloy Digest (1973) 22 (5): TS-254.
Published: 01 May 1973
... improved abrasion-resistance. Forms Available: Billets, forgings and bars. Applications: Die-casting dies, extrusion dies, trimmer dies, gripper dies, dummy blocks, hot-shear blades, and other similar hot-work applications Manufacturer: Bethlehem Steel Corporation Bethlehem, Pennsylvania 18016. ...
Journal Articles
Alloy Digest (1969) 18 (12): TS-225.
Published: 01 December 1969
... Pnblisbcd by Engineering Alloys Digest. Inc. Upper Montclair, New Jersey SPECIAL HS-55 (Hot-Work Tool Steel, Type H26) SPECIAL HS-55 is a hot-work tool and die .;tccI of the 18-4-l type of high-speed steel with lower carbon content for applications m which higher hardness must bc maintained at clcvutcd...
Journal Articles
Alloy Digest (1975) 24 (7): TS-289.
Published: 01 July 1975
... is relatively easy to machine, considering its high alloy content. It is rated at 65 as compared with a I-pet carbon tool steel which has a rating of 100. Workability: Bethlehem M-l can be hot worked readily by forging or rolling. The suggested forging temperature range is 1900 to 19500F. Do not hot work below...
Journal Articles
Alloy Digest (1962) 11 (12): TS-127.
Published: 01 December 1962
... and the furnace equipment used for heat treatment. Forms Available: Blanking and bending dies, master tools, forming rolls, broaches, drill bushings, knurling rools, master die and gauges, cold work tools, punches, cuctets. Manufacturer: Bethlehem Steel Company Bethlehem, Pennsylvania ...
Journal Articles
Alloy Digest (1971) 20 (7): CS-42.
Published: 01 July 1971
... Steel Corporation. Producer or Source: Bethlehem Steel Corporation Copyright ┬ę ASM International┬« 1996 1996 ASM International BETHLEHEM RQC-60 chemical composition corrosion-resistant alloys creep properties elasticity fatigue properties heat treatability joinability machinability...
Journal Articles
Alloy Digest (1976) 25 (9): TS-308.
Published: 01 September 1976
... readily in the annealed condition. Hot working presents no problems. Its scale can be removed by pickling or blasting. Its relatively high impact resistance, when tempered at 4000F or higher, is shown in Table 3. Forms Available: Bars, rods, plate and forgings. Applications: The following are some...