Alloy Digest (1978) 27 (8): SS-355.
Published: 01 August 1978
... BETHADUR 420 (AISI Type 420) is a 12.00 to 14.00% chromium stainless mold steel for plastics. Its good resistance to corrosion plus its working hardness level of Rockwell C 52 contribute to low maintenance costs for molds. This datasheet provides information on composition, physical properties...