Alloy Digest (1999) 48 (10): Cu-641.
Published: 01 October 1999
... Berylco 7 is beryllium copper alloy with 0.3% beryllium. The alloy has high conductivity, fatigue strength, and wear resistance and is nonmagnetic. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well asfatigue. Filing...
Journal Articles
Alloy Digest (1977) 26 (11): Ni-251.
Published: 01 November 1977
... BERYLCO Alloy 41C is a highly castable, air-melting nickel-base alloy; it is precipitation-hardenable to high strength and hardness. It exhibits excellent resistance to wear, corrosion and oxidation. Alloy 41C (formerly called Berylco CR-1, Alloy Digest Ni-27, September 1956) is the standard...
Journal Articles
Alloy Digest (1975) 24 (9): Ni-94.
Published: 01 September 1975
.... Machinability: BERYLCO 440 alloy is machinable with tungsten carbide tools using moderate speeds and light cuts. Better finishes can be obtained by increasing the speed and decreasing the feed. Suggested tool angles for single point tools are 5 to 7 degree end relief angle, a 15 to 30 degree side cutting edge...
Journal Articles
Alloy Digest (1973) 22 (1): Cu-264.
Published: 01 January 1973
... a rating of about 20%. Machining data are given in Tables 3 to 7. Workabili Hot workability of BERYLCO Alloy IO-52 is good. It can be hot forged or hot rolled at 1650 f 250F. Cold workability is excellent. Rod in the solution-annealed or cold-worked condition can be cold formed prior to age hardening...
Journal Articles
Alloy Digest (1973) 22 (9): Cu-271.
Published: 01 September 1973
... BERYLCO 25 is the standard high-performance beryllium copper alloy most widely used because of its high strength, hardness and excellent spring characteristics. BERYLCO 25 is the updated version of BERYLCO 25S (Alloy Digest Cu-3, November 1952). This datasheet provides information on composition...
Journal Articles
Alloy Digest (1954) 3 (7): Cu-18.
Published: 01 July 1954
... Berylco 20CR is the most widely used high strength beryllium copper casting alloy. This alloy can be heat treated to high hardness and tensile strengths; it has high impact strength and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1963) 12 (4): Cu-20.
Published: 01 April 1963
... Berylco 165 is a lower cost version of the standard 1.9 percent beryllium copper alloy. It offers good formability in the unhardened condition with high final properties following precipitation hardening. It is also available in the mill hardened condition which, without heat treatment...
Journal Articles
Alloy Digest (1956) 5 (2): Cu-35.
Published: 01 February 1956
... Berylco 275CR is a heat treatable beryllium copper casting alloy having high strength and hardness, and excellent corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture...
Journal Articles
Alloy Digest (1959) 8 (7): Cu-78.
Published: 01 July 1959
... BERYLCO 50 is a beryllium copper alloy offering high electrical conductivity and resistance to wear. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining...
Journal Articles
Alloy Digest (1956) 5 (9): Ni-27.
Published: 01 September 1956
... BERYLCO CR-1 is a high strength, corrosion resistant beryllium-nickel alloy which responds readily to an age-hardening heat treatment. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion...
Journal Articles
Alloy Digest (1967) 16 (7): Cu-178.
Published: 01 July 1967
... BERYLCO 717C is a high strength, age-hardenable copper-nickel casting alloy. It has high resistance to sea water corrosion and is recommended for marine equipment applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1958) 7 (2): Cu-59.
Published: 01 February 1958
... BERYLCO-10CR is a heat treatable, beryllium-copper casting alloy having high elastic and endurance strength, high ductility and impact strength, and high electrical and thermal conductivity. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1972) 21 (11): Ta-2.
Published: 01 November 1972
... temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ta-2. Producer or source: Kawecki Berylco Industries Inc.. See also Alloy Digest Ta-10, June 1988. Producer or Source: Kawecki Berylco Industries Inc. Copyright ┬ę ASM International┬«...
Journal Articles
Alloy Digest (1971) 20 (9): Be-1.
Published: 01 September 1971
... strength as well as fracture toughness and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Be-1. Producer or source: Kawecki Berylco Industries Inc.. Producer or Source: Kawecki...
Journal Articles
Alloy Digest (1952) 1 (3): Cu-3.
Published: 01 November 1952
... Berylco 25S alloy is the high-performance beryllium-copper spring material of 2 percent nominal beryllium content. It responds to precipitation-hardening for maximum mechanical properties. It has high elastic and endurance strength, good electrical and thermal conductivity, excellent resistance...