Alloy Digest (1978) 27 (5): Cu-353.
Published: 01 May 1978
... BELMONT Alloy 4582 is a alloy developed to meet the special needs of jewelers for a base-metal alloy suitable for casting centrifugally in refractory molds. It can be joined readily to itself and other alloys by soldering or brazing. This datasheet provides information on composition, physical...