Alloy Digest (1978) 27 (11): Bi-9.
Published: 01 November 1978
... BELMONT ALLOY 2505 is a bismuth-base, eutectic, low-melting alloy. It melts at 158 F and provides engineers and technicians with an easily castable material that is ready for use as soon as it freezes. Alloy 2505 can be recovered easily and recycled into new uses any number of times. Its many uses...
Journal Articles
Alloy Digest (1978) 27 (9): Bi-7.
Published: 01 September 1978
... pipe and tube exceed- ing approximately 1% to 2 inches in diameter prior to bending. (Belmont alloy 2505 is used for small diameter pipe and tube bending, but it is not strong enough for the heavy cross-section work.) Belmont alloy 2562 is also used to surround large cross-section moldings and channels...