Alloy Digest (1977) 26 (8): Al-228.
Published: 01 August 1977
... BELMONT ALLOY 1918 is a general-purpose aluminum casting alloy that can be sand cast and permanent-mold cast. It is used widely for bearings and is particularly suited for heavy-duty bearings such as those used for diesel engine crankshafts. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1977) 26 (10): Al-229.
Published: 01 October 1977
... for bearings and complex shapes. The castings are normally given a stabilizing thermal treatment identified as T5 temper. It is similar in composition to Belmont alloy 1918 except for the additional of nominally 2.5% silicon which contrbutes to an improvement of casting characteristics. The three greatest...