Journal Articles
Alloy Digest (1967) 16 (3): Al-164.
Published: 01 March 1967
... BA.704 is a heat treatable aluminum extrusion alloy having high tensile and fatigue strengths. It is recommended for aircraft components, gears, fittings and machinery parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1987) 36 (7): Be-5.
Published: 01 July 1987