Skip Nav Destination
Close Modal
Search Results for
BA.46
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-12 of 12 Search Results for
BA.46
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1955) 4 (3): Al-24.
Published: 01 March 1955
... BA.46 is a heat treatable aluminum casting alloy. It is recommended for high strength, pressure-tight castings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating...
Abstract
View article
PDF
BA.46 is a heat treatable aluminum casting alloy. It is recommended for high strength, pressure-tight castings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating and machining. Filing Code: Al-24. Producer or source: The British Aluminium Company Ltd.
Journal Articles
Alloy Digest (2001) 50 (8): SS-828.
Published: 01 August 2001
... is available in wide coil, sheet, or slit coil in widths up to 1250 mm, thickness 0.40 2.6 mm, and coil weights 8.0 9.0 kg/mm. The alloy is normally delivered in the fully softened and pinch/ skin passed condition. Alloy 430 can be supplied in a number of different surface finishes such as 2R (BA), 2B, matt...
Abstract
View article
PDF
AvestaPolarit 430 is a ferritic stainless steel with good corrosion resistance to the atmosphere, organic acids, detergents, and alkaline solutions. The alloy is easily formed and is used in decorative and trim work. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SS-828. Producer or source: AvestaPolarit AB.
Journal Articles
Alloy Digest (1955) 4 (1): SA-25.
Published: 01 January 1955
.../ C( 0-7OOOC) Modulus of elasticicy, psi 7.84 0284 0.000013% 3osxwOO PROPERTIES Table 1 -MINIMUM MECHANICAL PROPERTIES Thickness - inches N-2 incl over 2-4 incL over 46 incL Tensile srreng& psi 105000 105000 105000 Yidd s~engch, psi ( 0.2%) 9oooo 90000 Elongarioq % in 2 :; :i gYF Reduction of area...
Abstract
View article
PDF
CARILLOY T-1 is a low-carbon complex alloy steel used where high levels of yield strength and toughness are required. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: SA-25. Producer or source: United States Steel Corporation.
Journal Articles
Alloy Digest (2001) 50 (11): SS-837.
Published: 01 November 2001
... such as 2R (BA), 2B, matt, polished, or brushed. Applications: Typical applications include water heaters, heat exchangers, domestic appliances, sugar production tubing, and automotive exhaust components. Producer: AvestaPolarit 425 N. Martingale Rd., Suite 2000 Schaumburg, IL 60173 (800) 833-8703 (800) 545...
Abstract
View article
PDF
Avesta Polarit 430 Ti is a ferritic stainless steel with good high-temperature strength and an optimal weldability and formability. The alloy is not susceptible to chloride-ion stress-corrosion cracking, has good resistance to oxidation, and very good aqueous corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SS-837. Producer or source: AvestaPolarit AB.
Journal Articles
Alloy Digest (1999) 48 (4): Cu-632.
Published: 01 April 1999
... 42 27 16 37 3 4 hard 47 56 33 39 50 36 8 47 Hard 53 62 37 44 56 40 4 57 Extra-hard 59 65 41 46 60 43 2 60 Spring 64 71 45 50 66 47 1 min 62 min DOI: 10.31399/asm.ad.cu0632 than is required for C110 or C102. As a result, better formability is maintained at each temper (see Fig. 1). C151 has excellent...
Abstract
View article
PDF
Olin C151 is an age-hardenable dispersion strengthened zirconium-copper lead frame alloy. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, joining, and surface treatment. Filing Code: CU-632. Producer or source: Olin Brass.
Journal Articles
Alloy Digest (1955) 4 (4): Cu-25.
Published: 01 April 1955
... As Exuuded Light Anneal Hard Drawn (30%) Strength psi 54,000 54,000 60,000 70,000 54,000 72.000 52;ooo 56,000 74,000 Strength psi (0.5%) 21,000 21,000 35,000 50,000 21,000 50,000 20,000 23,000 55,000 445 :x :i 70 52 50 10 Rockwell I-hbCSS F B 30T 80 - 46 5% 2 - 75 67 80 - - - 78 - 78 - - 82 - 47 - 80 - 8.39...
Abstract
View article
PDF
MUNTZ METAL is a 60-40 copper-zinc alloy having good strength but low ductility. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Cu-25. Producer or source: Copper alloy mills.
Journal Articles
Alloy Digest (1989) 38 (5): CS-124.
Published: 01 May 1989
... ft/fV F (at 212 F) Thetmal coef. expansionPF (32-212 F) (32-752°F) (32-l 112°F) Elecuical resistivity, microhmcm (at 32OF) (at 2 12OF) Modulus of elasticity, psi PROPERTlES Table 1 -- TYPICAL. ROOM-TEMPERATURE UNHARDENED PROPERTIES -1 -in. Dia. Ba Annealed NOtTdhEd Hot Rolled (15500F. F C) to 1200°F...
Abstract
View article
PDF
UNS G10370 is a medium carbon, plain carbon steel. In bar form the steel is often used in the as-hot rolled condition. Cold drawn bars have attractive combinations of mechanical and dimensional properties and are widely used in mass production of machined and other parts. UNS G10370 is also used as a structural plate steel. See also Alloy Digest CS-127, June 1990. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: CS-124. Producer or source: Carbon steel mills.
Journal Articles
Alloy Digest (1954) 3 (1): Al-12.
Published: 01 January 1954
... S6 C-42 900 159,000 135.030 14.0 45.0 387 s4 c-41 1000 149.000 123.000 15.0 45.0 364 52 c-39 1100 1~7.000 120.000 16.5 47.0 340 48 C-36 1200 115,000 95.000 19.0 55.0 286 42 c-31 37.0 444 61 42.0 410 55 43.0 364 s2 47.5 348 48 54.0 298 42 i i i C-46 G42 c-39 c-37 c-31 Copyright © ASM International®...
Abstract
View article
PDF
BOHNALITE J is a high-copper aluminum alloy suitable for permanent mold and sand casting. It responds to heat treatment to produce high mechanical properties. It retains its strength well and has other excellent properties at elevated temperatures. Its bearing properties are also good. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high temperature performance as well as heat treating, machining, and joining. Filing Code: Al-12. Producer or source: Bohn Aluminum & Brass Corporation.
Journal Articles
Alloy Digest (1953) 2 (8): Cu-10.
Published: 01 August 1953
... Strength at 0.5% Extension % psi under Load : 0 46 :1 34.000 9, 37.000 19 41 19 44. f 47,000 53. 45,000 51, 2 2 70 51 54,000 8 51,000 5 6 g: 71: g Cold rolling to indicated thickness reduction followed a soludon anneal (3/4 hour at 975X1000°C) and quench. Variations in prop- erties must be expected...
Abstract
View article
PDF
Chromium Copper-999 is a copper-chromium-silicon alloy which is softened by a high-temperature solution anneal and quench, and will acquire improved properties with a low-temperature precipitation heat treatment. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and creep. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Cu-10. Producer or source: American Brass Company.
Journal Articles
Alloy Digest (1998) 47 (10): TS-561.
Published: 01 October 1998
.... More information on both grinding and machinin8 (turning, drilling, milling) is available from the producer. Table 3 Wheel Selection Annealed Type of grindiig condition Hardened condition Face arinding, straight wheel 46 NV BI51 R75B3(a),3SG46HVSA46GV Face &ui& w&ems 24 GV 3SG36HVS(bj,A36HV CyIiadricaI...
Abstract
View article
PDF
Vanadis 23 is a Cr-Mo-W-Va alloyed high-speed steel made by powder metallurgy. The tool steel offers an excellent combination of wear resistance and toughness. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on heat treating, machining, and surface treatment. Filing Code: TS-561. Producer or source: Uddeholm Corporation. See also Alloy Digest TS-552, March 1997.
Journal Articles
Alloy Digest (1971) 20 (5): TS-233.
Published: 01 May 1971
... SIZE ON CORE PROPERTIES (Compamon. 70: 0.10 C, 0.40 Mn. 3.25 Ni, 1.50 CrJ fTw,ner are for ba, cemenl 0.283 7.85 7.1 x 10-6 28x106 12x106 Tensile Roprues BU TCIllpflng Tellnle Yield El0ngr- Reduction Diamewr Tempenturr BIlllCll SIEilgth Polnr 0 of Alea A-- OF HudIle% zz-- % 90 !,i 300 341 l72OOO...
Abstract
View article
PDF
AISI Type P6 is a low-carbon, high-hardenability steel which is carburized and used for molding plastics. It develops a strong, wear-resistant case combined with a hard, tough core and is recommended for the most demanding mold requirements. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-233. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1993) 42 (3): Co-90.
Published: 01 March 1993
...) w-t Rockwell C Room pJM 125 (863) cl 54 cast 79 (545) cl 54 P/M loo0 (538) C.t 105 (725) Cl 46 72 (497) Cl 45 1200 (649) ;Et 100 (690) <l 39 70 (483) <l 38 P/M 1400(7fw cast 90 (621) 1 70 (483) <l *Maximlml 28 27 Table 3 -TRANSVERSE RUPTURE STRENGTH ksi (MPa) P/M - 149 (966) cast - Table 4...
Abstract
View article
PDF
STELLITE 3 PM (UNS R30103) is a cobalt-base alloy recommended for handling severe conditions of abrasion, heat and corrosion. The PM designation indicates prealloyed atomized powders and parts made from the powder. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on wear resistance as well as heat treating, machining, joining, and powder metal forms. Filing Code: CO-90. Producer or source: Deloro Stellite Inc.