1-20 of 2982 Search Results for

B

Sort by
Journal Articles
Alloy Digest (2017) 66 (4): Cu-860.
Published: 01 April 2017
... Bearium B-4, B-8, B-10, and B-11 are copper-base, high-lead bearing bronzes with superior resistance to scoring and seizure beyond the endurance and danger limits of ordinary bearing bronzes. It is used in applications involving high speeds, poor lubrications, heat-generating loads, elevated...
Journal Articles
Alloy Digest (1985) 34 (10): TS-448.
Published: 01 October 1985
... SELECT B is a fully uniform air-hardening die steel having abrasion resistance intermediate between Olympic (AISI Type D2) high-carbon, high-chromium die steel and Badger (AISI Type O1) oil-hardening die steel. SELECT B has excellent non-deforming, deep-hardening characteristics and good toughness...
Journal Articles
Alloy Digest (1986) 35 (10): Fe-73.
Published: 01 October 1986
... CMI-B Magnetic Iron is an ultra-low-carbon magnetic iron especially processed for good magnetic properties and processability. It is used for relays and other electromagnetic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1988) 37 (9): Ni-362.
Published: 01 September 1988
... BRIGHTRAY Alloy B is an electrical resistance wire which contains rare-earth long-life additions. It is useful up to 1100 C (2010 F). It has a greater temperature coefficient of resistance than the essentially binary 80/20 nickel chromium resistance grade. It is suitable for less exacting...
Journal Articles
Alloy Digest (1988) 37 (10): Ni-363.
Published: 01 October 1988
... JESSOP JS Alloy B-2 is a nickel-molybdenum alloy with outstanding corrosion resistance in the as-welded condition. It can be used up to 1000 F and, with proper atmospheric protection, above 1500 F. In the range 1000-1500 F the alloy exhibits reduced ductility and use in that temperature range...
Journal Articles
Alloy Digest (2003) 52 (10): Ti-131.
Published: 01 October 2003
... ASTM B 367 GRADE C-3 is a commercially pure titanium casting alloy. For the most part, titanium casting alloys are based on traditional wrought product compositions. Several data sheets for commercially pure (CP) grades of wrought titanium alloys have been published in Alloy Digest. This data...
Journal Articles
Alloy Digest (2003) 52 (10): Zr-11.
Published: 01 October 2003
... ASTM B 752 GRADE 702C is a zirconium casting alloy. Zirconium alloys are extremely corrosion resistant. They are expensive, but in some cases are superior in corrosion performance to stainless steels, nickel alloys, and titanium. The largest application for zirconium castings is handling...
Journal Articles
Alloy Digest (2003) 52 (11): Ti-132.
Published: 01 November 2003
... ASTM B 367 GRADE Ti-Pd8A is commercially pure titanium casting alloy with a small palladium addition. For the most part, titanium casting alloys are based on traditional wrought product compositions. The small palladium addition to this grade improves corrosion resistance while not changing any...
Journal Articles
Alloy Digest (2003) 52 (11): Zr-12.
Published: 01 November 2003
... ASTM B 752 Grade 705C zirconium casting alloy is basically identical in composition and similar in properties to its wrought equivalent, UNS R60705, which is grade 705. Zirconium alloys are expensive, but are more corrosion resistant than stainless steels, nickel alloys, and titanium. The largest...
Journal Articles
Alloy Digest (1997) 46 (1): Cu-609.
Published: 01 January 1997
... Magnolia B-1 is a lead-free copper alloy. It machines easier than the leaded SAE 660 alloy that it was designed to duplicate. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1998) 47 (1): Fe-116.
Published: 01 January 1998
... Carpenter Silicon Core Iron B-FM is melted in electrical arc furnaces to exacting chemical specifications and is carefully controlled in rolling and annealing practices to produce a fine-grained uniform quality magnetic core alloy. Silicon Core Iron B-FM has improved machining characteristics over...
Journal Articles
Alloy Digest (1999) 48 (5): Ni-552.
Published: 01 May 1999
... Hastelloy B-3 alloy welding products are used to promote similar corrosion resistance to Hastelloy B-3 (Alloy Digest Ni-461, August 1994) and B-2 (Alloy Digest Ni-249, September 1997) base metals, for the dissimilar welding of Hastelloy B-3 and B-2 to nickel or iron-base corrosion resistant alloys...
Journal Articles
Alloy Digest (1968) 17 (8): Fe-35.
Published: 01 August 1968
... B and W IRON is a thoroughly killed, low carbon steel having a combination of ductility, toughness and high magnetic permeability. It is recommended for applications where good magnetic characteristics are of primary significance, such as in the manufacture of electric motor and generator housings...
Journal Articles
Alloy Digest (1969) 18 (8): Ni-146.
Published: 01 August 1969
... ILLIUM B was developed as a bearing alloy for maximum wear and galling resistance in high concentrations of hot sulfuric acid. The alloy is capable of being age hardened. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1969) 18 (9): SA-244.
Published: 01 September 1969
... UDIMAR B-300 is an 18% nickel maraging steel having excellent toughness and ductility at high strength levels. It is a fabricable and weldable ultra-high strength alloy steel combining the mechanical properties derived from precipitation hardening and martensitic transformation. It has increased...
Journal Articles
Alloy Digest (1970) 19 (1): SA-248.
Published: 01 January 1970
... HY-TEN B Temper No. 3X-40 is a medium-carbon alloy steel having free-cutting characteristics. It is recommended for machine tools, mining and road building equipment, gears, crankshafts, bolts, etc. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1955) 4 (5): TS-33.
Published: 01 May 1955
... JESSOP 2-B is a general purpose hot work die steel having great resistance to abrasion. It is supplied in three grades. namely 2-B (L.C.), 2-B (M.C.) and 2-B (H.C.). These are classed as ASM Type IV F1, Type IV F3 and Type IV F2 respectively. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1955) 4 (6): CS-3.
Published: 01 June 1955
... MAX-EL 1-B offers a case hardening grade of excellent machining characteristics, plus good mechanical properties in the core with minimum distortion during heat treatment. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1960) 9 (8): Al-94.
Published: 01 August 1960
... CERALUMIN-B is an age-hardenable general purpose aluminum casting alloy having good high temperature properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on high...
Journal Articles
Alloy Digest (1960) 9 (9): SA-103.
Published: 01 September 1960
... HY-TEN B TEMPER No. 3-X is a strong, tough alloy steel of high hardenability recommended for heavy duty applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information...