Alloy Digest (2012) 61 (5): TS-702.
Published: 01 May 2012
... Böhler K294 Microclean is a powder metallurgically produced cold work tool steel. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on heat treating and powder metal forms. Filing Code: TS-702. Producer or source: Böhler...