Skip Nav Destination
Close Modal
Search Results for
Böhler K110
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
Böhler K110
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2020) 69 (12): TS-805.
Published: 01 December 2020
... Böhler K110 is a high-carbon, Cr-Mo-V, alloy cold-work tool steel that is suitable for medium-run tooling where abrasive wear is dominant and the risk of chipping or cracking is not high. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also...
Abstract
View article
PDF
Böhler K110 is a high-carbon, Cr-Mo-V, alloy cold-work tool steel that is suitable for medium-run tooling where abrasive wear is dominant and the risk of chipping or cracking is not high. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming and heat treating. Filing Code: TS-805. Producer or source: voestalpine Böhler Edelstahl GmbH&Co KG.