Alloy Digest (2016) 65 (1): TS-733.
Published: 01 January 2016
... Böhler (or Boehler) M268 VMR is a hardened and tempered plastic mold steel with excellent cleanliness for best polishing. This datasheet provides information on composition, physical properties, microstructure, and elasticity. It also includes information on forming, heat treating, and joining...