Alloy Digest (2016) 65 (2): TS-734.
Published: 01 February 2016
... Böhler (or Boehler) K490 Microclean is an improved and more efficient cold work tool steel compared with other commonly used PM steels such as M4 or PM23. Toughness is more than doubled with a similar wear resistance. This datasheet provides information on composition and physical properties as...
Journal Articles
Alloy Digest (2017) 66 (4): TS-740.
Published: 01 April 2017
... Böhler (or Boehler) K490 Microclean is a PM cold work tool steel that has a combination of wear resistance and high toughness. It is made by powder metallurgy. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on wear...