Skip Nav Destination
Close Modal
Search Results for
Austral Wright C26000 (70-30 Brass)
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
Austral Wright C26000 (70-30 Brass)
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2024) 73 (9): CU-944.
Published: 05 September 2024
... Austral Wright C26000 (70-30 Brass) is a copper-zinc alloy. It has the distinctive clear bright yellow color normally associated with brass. Austral Wright C26000 possesses an excellent combination of strength and ductility. This grade is the most widely available copper alloy in the sheet form...
Abstract
View article
PDF
Austral Wright C26000 (70-30 Brass) is a copper-zinc alloy. It has the distinctive clear bright yellow color normally associated with brass. Austral Wright C26000 possesses an excellent combination of strength and ductility. This grade is the most widely available copper alloy in the sheet form. It is often used where its deep drawing qualities are needed. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-944. Producer or source: Austral Wright Metals.