Alloy Digest (2022) 71 (2): Cu-929.
Published: 01 February 2022
... Austral Wright 5% Phosphor Bronze (UNS C51800) is a wrought copper-tin-phosphorus alloy. It is the most widely used grade of wrought phosphor bronze. It is harder, stronger and stiffer than the wrought brasses and, in strip and wire form, is produced with a combination of excellent cold...