Alloy Digest (2023) 72 (9): Cu-941.
Published: 01 September 2023
... Aurubis CuSn0.15 is a tin bearing copper that combines medium strength with good electrical and thermal conductivity. Moreover, the alloy exhibits an increased temperature stability as compared to the highest conductive copper alloys. This datasheet provides information on composition, physical...