Skip Nav Destination
Close Modal
Search Results for
Aurubis Cu-OFE
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
Aurubis Cu-OFE
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2020) 69 (4): Cu-907.
Published: 01 April 2020
... Aurubis Cu-OFE (oxygen-free electronic) is an oxygen-free, high conductivity copper with 99.99% minimum copper. It offers the advantages of both electrolytic tough pitch (ETP) copper and phosphorus deoxidized (DHP) copper. Its high purity, with less than 5 ppm (0.0005%) oxygen, and the absence...
Abstract
View article
PDF
Aurubis Cu-OFE (oxygen-free electronic) is an oxygen-free, high conductivity copper with 99.99% minimum copper. It offers the advantages of both electrolytic tough pitch (ETP) copper and phosphorus deoxidized (DHP) copper. Its high purity, with less than 5 ppm (0.0005%) oxygen, and the absence of deoxidizers accounts for minimum 101% IACS electrical conductivity as well as no susceptibility to hydrogen embrittlement. Cu-OFE has very good formability and can be soldered and welded, which makes it superior to Cu-ETP in these aspects. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and machining. Filing Code: Cu-907. Producer or source: Aurubis AG.