Alloy Digest (2022) 71 (1): Cu-928.
Published: 01 January 2022
... Aurubis Cu-DLP is a phosphorus-deoxidized copper that contains a minimum of 99.90% copper and a small amount of residual phosphorus. Owing to the presence of residual phosphorus, the electrical conductivity of Aurubis Cu-DLP is lower than that of the high-conductivity and oxygen-free coppers (Cu...