1-1 of 1 Search Results for

Atlas KK

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1962) 11 (5): SA-128.
Published: 01 May 1962
... Atlas KK has been especially designed for those machinery applications that require a file-hard wearing surface with reasonable toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...