1-1 of 1 Search Results for

Atlas 5251

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2022) 71 (1): Al-484.
Published: 01 January 2022
... Atlas 5251 is a wrought, non-heat-treatable, aluminum-magnesium alloy (5xxx series). Alloy 5251, registered in 1972, is essentially the same as the old N4 alloy and is produced primarily in Europe for a variety of common alloy applications. It offers properties similar to those of alloy 5052...