Alloy Digest (2019) 68 (12): SA-858.
Published: 01 December 2019
... Armstrong Ultra 690 is a high yield strength steel for welded and weight saving in structures. It has a minimum yield strength of 690 MPa (100 ksi) in thicknesses up to 50 mm (2 in.). This datasheet provides information on composition and tensile properties. It also includes information on forming...