Journal Articles
Alloy Digest (1962) 11 (1): SA-123.
Published: 01 January 1962
... Armco High Strength No. 2 is a high-strength low-alloy steel designed to give excellent corrosion resistance coupled with superior mechanical properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1976) 25 (1): SS-324.
Published: 01 January 1976
... NITRONIC 33 is characterized by (1) High yield strength, (2) Good resistance to stress-corrosion cracking, (3) Low magnetic permeability even after severe cold working, (4) Excellent strength and ductility at cryogenic temperatures, and (5) Good resistance to wear and galling; in fact...
Journal Articles
Alloy Digest (1964) 13 (9): SA-168.
Published: 01 September 1964
... without pre- or post-heating. However, because of its composition, it is not as satis- factory for resistance welding as Armco High Strength No. 1 or No. 2. Can be welded under ordinary conditions by the metal-arc welding process in thicknesses up to and including 1 ;2 inch without recourse to an) special...
Journal Articles
Alloy Digest (1987) 36 (4): SS-484.
Published: 01 April 1987
.... Average of duplicate tests. **ALUMINIZED STEEL is a registered trademark of Armco Inc. Table 5 - COMPARATIVE ROOM-TEMPERATURE PROPERTIES AFTER 1006 HOURS AT 900┬░F Condition Tensile Strength psi Yield Strength (0.2% Offset) psi Elongation (2 in.; 50.8 mm) 9% Rockwell B Hardness ARMCO I8Cr-Cb HIGH...
Journal Articles
Alloy Digest (1979) 28 (3): SA-356.
Published: 01 March 1979
... ARMCO FORMABLE 50 HR is a hot-rolled high-strength low-alloy steel that provides excellent ductility, weldability and edge-tear resistance at a minimum yield strength of 50,000 psi (345 MPa). It has unusually good fabricating properties that are the result of closely controlled processing...
Journal Articles
Alloy Digest (1979) 28 (5): SA-359.
Published: 01 May 1979
... ARMCO FORMABLE 70 HR is a hot-rolled steel with excellent ductility, weldability and edge-tear resistance at a minimum yield strength of 70,000 psi (483 MPa). For this relatively high strength level, it has unusually good fabricating properties that are the result of closely controlled processing...
Journal Articles
Alloy Digest (1986) 35 (12): SS-479.
Published: 01 December 1986
...(505) 8 I 300( 560) 96400(665) 102 lOO(704) *Annealed. Elongation Rockwell (2 in.: 50.8 mm) B % Hardness 35.8 69.2 25.2 83.5 16.0 87.0 9.5 90.8 - 95.8 3.0 97.2 Table 4 - SHORT-TIME ELEVATED-TEMPERATLIRE STRENGTH OF ARMCO 409 HIGH PERFORMPINCE-IO AND TWO OTHER MATERIALS ARMCO 409 HIGH PERFORMANCE-IO...
Journal Articles
Alloy Digest (1987) 36 (6): SS-486.
Published: 01 June 1987
... ARMCO 439 HIGH PERFORMANCE-10 is a ferritic stainless steel sheet and strip alloy suited to automotive-exhaust system applications where oxidatin resistance is needed at temperatures beyond the capability of AISI Type 409 to withstand. The alloy also has good resistance to wet chloride...
Journal Articles
Alloy Digest (1973) 22 (2): SS-286.
Published: 01 February 1973
... ARMCO 18-3Mn is a low-nickel stainless steel having a high yield strength, low magnetic permeability in all conditions and good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1961) 10 (12): SS-125.
Published: 01 December 1961
... Armco 21-6-9 is an austenitic stainless steel alloy designed for use in applications where a combination of high strength and corrosion resistance is desired. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Journal Articles
Alloy Digest (1971) 20 (3): SS-252.
Published: 01 March 1971
... by Engineering Alloys Digest, Inc. Upper Moncchir, New Jersey ARMCO 22-13-5* (High-Strength, Corrosion-Resistant Austenitic Stainless Steel) ARMCO 22-13-5 provides an unusually good combination of corrosion resistance and strength for an austenitic stainless steel. It is nonmag- netic even after severe cold work...
Journal Articles
Alloy Digest (1971) 20 (2): SA-260.
Published: 01 February 1971
... ARMCO VNT is a high-strength, low-alloy steel normalized for added toughness, ductility and uniformity. It is a silicon-killed, vanadium-nitrogen treated steel, made to fine-grain practive and provides a 60,000 psi minimum yield strength. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1981) 30 (5): SA-380.
Published: 01 May 1981
... ARMCO SSS 100A is a low-carbon, fine-grained, quenched-and-tempered alloy steel. It is strong, tough and readily fabricated with equipment and facilities suited to its high strength. It has a minimum yield strength of 100,000 psi. Among its many uses are structural components in heavy-duty...
Journal Articles
Alloy Digest (1961) 10 (5): SA-115.
Published: 01 May 1961
... across the rolling direction, flanging and light forming operations of the type regularly performed by standard commer- cial quality sheets and plates. For more dif- ficult forming operations, consideration should be given to using Armco High Strength No.2. Weldability: All types ofwelding are possible...
Journal Articles
Alloy Digest (1971) 20 (6): SS-255.
Published: 01 June 1971
... ARMCO 18-2 Mn is a low-nickel austenitic stainless steel that has a yield strength approximately twice that of Type 304 stainless steel as well as comparable corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1986) 35 (3): SA-415.
Published: 01 March 1986
... using MIG. TIG and high-frequency procedures similar to those used with Type 409 stainless. The recommended wire. when requtred. is I8 Cr-Cb with 409 Cb a suggested alternative. ARMCO ULTRA-THERM 1600 may also be resistance seam or spot welded. The mechanical strength of the weld can be as good...
Journal Articles
Alloy Digest (1968) 17 (12): SA-234.
Published: 01 December 1968
... ARMCO SSS-100 is a quenched and tempered low-carbon, alloy constructional steel providing high strength, exceptional notch toughness, good weldability and improved atmospheric corrosion resistance along with good abrasion resistance. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1978) 27 (7): SA-348.
Published: 01 July 1978
... or transverse direction with a bend radius of 2t (t = plate thickness). Welding: Armco N&COP steel is readily welded with the Submerged Arc (SAW), Shielded Metal-Arc (SMAW) and Gas Metal-Arc (GMAW) welding processes using com- mercially available welding materials. Compared to conventional high-strength low...
Journal Articles
Alloy Digest (1972) 21 (3): Ni-169.
Published: 01 March 1972
..., elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-169. Producer or source: Armco Steel Corporation, Advanced Materials...
Journal Articles
Alloy Digest (1989) 38 (5): SS-3.
Published: 01 May 1989
... ARMCO 17-7 PH is a precipitation-hardening stainless steel that provides high strength and hardness, excellent fatigue strength, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition, then hardens to high strength levels by simple heat...