Alloy Digest (1970) 19 (10): SS-49.
Published: 01 October 1970
... ARMCO 22-4-9 is an austenitic stainless steel that provides high hot hardness, and retains this hardness at elevated temperatures. In addition, it has good and room and elevated temperature mechanical properties, as we as good oxidation resistance, stress rupture and creep characteristics...
Journal Articles
Alloy Digest (1987) 36 (4): SS-484.
Published: 01 April 1987
... 777 1022 ALUMINIZED STEEL, Type I** 22.I 36.8 65.4 117 152 Discontinued AISI Type 409 18.3 93.9 310 Discontinued ARMCO 18Cr-Cb HIGH PERFORMANCE-IO 0.9 1.0 I.1 1.1 1.2 I.3 1.4 1.5 1.4 1.2 1.2 0.8 AISI Type 304 I.1 1.2 I.1 -9.8 -36.4 -II2 -710 Discontinued *Cycle: 25 minutes heat, 5 minutes cool...
Journal Articles
Alloy Digest (1990) 39 (8): SS-327.
Published: 01 August 1990
... ARMCO NITRONIC 40 Stainless Steel is one of the most versatile austenitic stainless steels with a room-temperature yield strength about twice that of AISI Types 304, 321 and 347. In addition, NITRONIC 40 has remarkably good elevated temperature properties and oxidation resistance. It retains high...
Journal Articles
Alloy Digest (1981) 30 (5): SA-380.
Published: 01 May 1981
... is recommended. Estensive details on welding are available from the manufacturer as weU as alloy electrode wires for submerged- arc welding with basic neutral-type fluxes. Corrosion Resistance: The atmospheric corrosion resistance of Armco SSS 1OOA is 2 t6 4 times that of carbon steel without copper...
Journal Articles
Alloy Digest (1986) 35 (11): SS-477.
Published: 01 November 1986
...-lb 5 2 ft-lb J 33 44 38 I20+ 163+ 23 31 30 41 - - I3 I8 20 27 8 II I6 22 ii - II9 5 7 I2 16 71 96 4 5 7 9 - - 4 5 4 5 30 41 Heat Treatment: Solution Treatment: CARPENTER PH 13-8 MO may be solution treated at I7OO F for a time dependent on section size but normally one hour. followed by air cooling...