Alloy Digest (1954) 3 (8): CI-7.
Published: 01 August 1954
... ArmaSteel is a cast ferrous alloy possessing the advantages of high yield strength, excellent wear resistance, and adaptability to selective hardening. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...