Journal Articles
Alloy Digest (1970) 19 (6): Al-197.
Published: 01 June 1970
... resistance as well as casting, heat treating, and machining. Filing Code: Al-197. Producer or source: Arwood Corporation. Producer or Source: Arwood Corporation Copyright Ā© ASM InternationalĀ® 1996 1996 ASM International Arcast 67 castability chemical composition corrosion-resistant alloys...